Paramount Instruments Pilling Tester With 2 Boxes is a fabric testing instrument, still in its builder’s current range. Its builder lists drum speed 60 rpm, chamber count 2 chamber and weight 55kg (121 lb). Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.

Fabric testingTesting and laboratoryIn the builder's current range

Specification

ParameterValue
Tester TypeICI type
Chamber Count2 chamber
Drum Speed60 rpm
Weight55kg (121 lb)
Length8280 mm (32 1/2 Inch)
Depth518 mm (20 1/2 Inch)
Height508 mm (20 Inch)
International standardsBS EN ISO 12945-1-BS 5811-WSTM 152-Next 19, CE

Read from the builder's published page: www.paramountinstruments.in, on 2026-11-16.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.paramountinstruments.in,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device