Q-Lab Q-SUN Xe-3 is a fabric testing instrument, still in its builder’s current range. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability. They test fabric from weaving and knitting through finishing and garment making, checking compliance with buyer and standard specifications.
Checked against the builder's page. On 2026-11-18 an automated check found every figure on this record on the builder's page, www.q-lab.com, and the page names this model. No editor has reviewed it; confirm against the source before sizing or ordering.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 0 of 5 key figures recorded
- Test performed—
- Measuring range—
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Make
- Q-LabUnited Statesq-lab.com (the builder's website, opens in a new tab) All 5 machines from Q-Lab
- Class
- Fabric testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
Specification
| Parameter | Value |
|---|---|
| Lamps | three lamps per machine |
| Lamp life | 3000 hours at normal irradiance and 1000 hours at high irradiance |
| Black panel temperature range | between 42 °C and 120 °C |
| Specimen tray | 451 × 718 mm (17.8 × 28.3 in), holds up to 55 specimens @ 51 × 102 mm (2 × 4 in) |
| Irradiance control | 340 nm, 420 nm, or TUV (Total UV, 300-400 nm) |
Read from the builder's published page: www.q-lab.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.q-lab.com,
- Last changed
Related machines
Also from Q-Lab
Other machines of this kind: Fabric testing
Report incorrect information on this page