Taber Industries 150-T V-5 Stiffness Tester is a fabric testing instrument, still in its builder’s current range. Its builder lists range weights 500, 1000 and 2000 Taber Units, measuring range up to 10,000 Taber and specimen thickness 0.004" to 0.297". Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Test performed—
- Measuring rangeup to 10,000 Taber Stiffness Units
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Make
- Taber IndustriesUnited Statestaberindustries.com (the builder's website, opens in a new tab) All 6 machines from Taber Industries
- Class
- Fabric testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
Specification
| Parameter | Value |
|---|---|
| Measuring range | up to 10,000 Taber Stiffness Units |
| Accuracy | ±1.0% |
| Specimen thickness | 0.004" to 0.297" |
| Number of test ranges | Nine (9) |
| Deflection angle | 7 1/2° or 15° |
| Range weights | 500, 1000 and 2000 Taber Units |
| Optional range weight set | 3000 and 5000 Taber units |
| Wire/cable specimen | 70mm long and 3mm - 8mm in diameter |
| Power supply | 115/230V, 50/60Hz |
Read from the builder's published page: www.taberindustries.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.taberindustries.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Taber Industries
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.