Taber Industries 5820 Webbing Abrasion Tester is a fabric testing instrument, still in its builder’s current range. Its builder lists maximum stroke length 305mm (12 inch), standard weight set 2, 4 & 5.2 lbs. and specimen angle to hex bar 85° (±2°). Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Test performedAbrasion resistance of seat belts and webbing
- Measuring range—
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Rubbing / friction stroke305 mm
- Make
- Taber IndustriesUnited Statestaberindustries.com (the builder's website, opens in a new tab) All 6 machines from Taber Industries
- Class
- Fabric testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
Specification
| Parameter | Value |
|---|---|
| Test performed | Abrasion resistance of seat belts and webbing |
| Specimen angle to hex bar | 85° (±2°) |
| Number of specimens | up to three |
| Maximum stroke length | 305mm (12 inch) |
| Speeds | 15, 30, 37, 45, and 60 cycles per minute |
| Standard weight set | 2, 4 & 5.2 lbs. |
| Optional weight set | 3 & 5 lbs. |
| Breaking strength capacity | over 13,500 N |
Read from the builder's published page: www.taberindustries.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.taberindustries.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Taber Industries
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.