Thwing-Albert Instrument Handle-O-Meter is a fabric testing instrument, still in its builder’s current range. Its builder lists power - standard 115 V ±10%, 60 Hz and net weight 22.2 kg (49 lb). Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 2 of 5 key figures recorded
- Test performedSoftness/handle (stiffness plus surface friction) of nonwovens, textiles
- Measuring range0–100 grams
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Weight22.2 kg
Specification
| Parameter | Value |
|---|---|
| Test performed | Softness/handle (stiffness plus surface friction) of nonwovens, textiles |
| Measurement Range - Standard Unit | 0–100 grams |
| Measurement Range - Heavy Duty Unit | 0–1,000 grams |
| Measurement Resolution - 100g Beam | 0.1 gram |
| Measurement Resolution - 1,000g Beam | 1 gram |
| Slot Opening Options | 5 mm, 10 mm, 20 mm, 1/4 in, 3/8 in |
| Test Modes | Single, Double, Quadruple (with automatic averaging) |
| Power - Standard | 115 V ±10%, 60 Hz |
| Dimensions (D × W × H) | 368 mm × 587 mm × 229 mm (14.5″ × 23 1/8″ × 9″) |
| Net Weight | 22.2 kg (49 lb) |
| Industry Standards | ASTM D6828-02, INDA IST 90.3, NWSP 090.3.R0 |
Read from the builder's published page: www.thwingalbert.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.thwingalbert.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Thwing-Albert Instrument
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.