Thwing-Albert Instrument QC-3A is a fabric testing instrument, still in its builder’s current range. Its builder lists capacity 1100 lbs (5 kN/500 kg), net weight 180 lbs (82 kg) and horizontal clearance 13.5 inches (34 cm). Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Checked against the builder's page. On 2026-11-17 an automated check found every figure on this record on the builder's page, www.thwingalbert.com, and the page names this model. No editor has reviewed it; confirm against the source before sizing or ordering.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Test performedTensile, compression, coefficient of friction and peel
- Measuring range—
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Force capacity0–5 N
- Weight81.6 kg
Specification
| Parameter | Value | Comparable |
|---|---|---|
| Test performed | Tensile, compression, coefficient of friction and peel | |
| Capacity | 1100 lbs (5 kN/500 kg) | |
| Crosshead Speed | 0.1 – 20 in/min (2.54 – 508 mm/min) | |
| Horizontal Clearance | 13.5 inches (34 cm) | |
| Force Reading Accuracy | ±0.25% Measuring Value (10% to 100% load capacity) | |
| Load cell capacities | 0 to 5 N up to 0 to 5000 N | |
| Net Weight (10" travel) | 180 lbs (82 kg) | 81.6 kg |
| Power Requirements | 110V 50 or 60Hz, 220V 50Hz, 230V 50Hz, 240V 50Hz |
Read from the builder's published page: www.thwingalbert.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.thwingalbert.com,
- Last changed
Related machines
Also from Thwing-Albert Instrument
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.