Man-made fibres regulations by market
7 obligations that name man-made fibres in their scope, from 7 instruments across 2 markets, soonest date first, each stating how firm its date actually is.
The instruments (7)
| Instrument | Citation | Market | Made by | Status |
|---|---|---|---|---|
| India 100 Percent Polyester Spun Grey and White Yarn QCO 2023 (rescinded) | S.O. 3195(E) | IN | Ministry of Chemicals and Fertilizers (Department of Chemicals and Petrochemicals) | Repealed |
| India Polyester Continuous Filament Fully Drawn Yarn QCO 2023 (rescinded) | S.O. 3193(E) | IN | Ministry of Chemicals and Fertilizers (Department of Chemicals and Petrochemicals) | Repealed |
| India Polyester Industrial Yarn QCO 2022 (rescinded) | S.O. 1652(E) | IN | Ministry of Chemicals and Fertilizers (Department of Chemicals and Petrochemicals) | Repealed |
| India Polyester Partially Oriented Yarn QCO 2023 (rescinded) | S.O. 3194(E) | IN | Ministry of Chemicals and Fertilizers (Department of Chemicals and Petrochemicals) | Repealed |
| India Polyester Staple Fibres QCO 2022 (rescinded) | S.O. 1651(E) | IN | Ministry of Chemicals and Fertilizers (Department of Chemicals and Petrochemicals) | Repealed |
| India Viscose Staple Fibres QCO 2022 (rescinded) | S.O. 6143(E) | IN | Ministry of Textiles | Repealed |
| US OCPSF Effluent Guidelines | 40 CFR Part 414 | US | Environmental Protection Agency | In force |
Already in force 6
-
India Polyester Industrial Yarn QCO 2022 (rescinded) S.O. 1652(E) IN
The Polyester Industrial Yarn (Quality Control) Order, 2022, which made IS 17264:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5132(E) of 12 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
-
India Polyester Continuous Filament Fully Drawn Yarn QCO 2023 (rescinded) S.O. 3193(E) IN
The Polyester Continuous Filament Fully Drawn Yarn (Quality Control) Order, 2023, which made IS 17261:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5134(E) of 12 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
-
India Polyester Partially Oriented Yarn QCO 2023 (rescinded) S.O. 3194(E) IN
The Polyester Partially Oriented Yarn (Quality Control) Order, 2023, which made IS 17262:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5135(E) of 12 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
-
India 100 Percent Polyester Spun Grey and White Yarn QCO 2023 (rescinded) S.O. 3195(E) IN
The 100 Percent Polyester Spun Grey and White Yarn (Quality Control) Order, 2023, which made IS 17265:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5131(E) of 12 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
-
India Polyester Staple Fibres QCO 2022 (rescinded) S.O. 1651(E) IN
The Polyester Staple Fibres (Quality Control) Order, 2022, which made IS 17263:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5133(E) of 12 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
-
India Viscose Staple Fibres QCO 2022 (rescinded) S.O. 6143(E) IN
The Viscose Staple Fibres (Quality Control) Order, 2022, which made IS 17266:2019 and the BIS Standard Mark compulsory, was rescinded by S.O. 5267(E) of 18 November 2025 with immediate effect. The Standard Mark is no longer required by law; the Indian Standard can still be specified by contract.
Confirmed In force, dates fixed in published law
No date set 1
-
no date set
US OCPSF Effluent Guidelines 40 CFR Part 414 US
Process wastewater discharges from establishments manufacturing organic chemicals, plastics and synthetic fibres covered by the part's subparts are subject to its effluent limitations and pretreatment standards.
Confirmed In force, dates fixed in published law
This is the upstream of a synthetic spinner rather than the spinner itself: the rayon, other fibres and thermoplastic resin subparts are where polyester and viscose production sit. The record carries the general duty the part imposes. It does not enumerate the individual disclosures, exemptions and test conditions, which run to dozens of sections in the part itself.