Yarns are continuous strands of fibers that can be woven or knitted into fabrics. Natural staple fibers usually requires processes such as spinning to make yarns. Silk yarn, extracted from silk cocoon are continuous filament yarns. Most of…
Read More...
Read More...
Twist insertion and Different Spinning Techniques
The new spinning systems clearly avoid the limitations produced by the twist insertion mechanism. It is possible to increase the twist insertion rate and the yarn production speed quite considerable. Various spinning techniques…
Read More...
Read More...
Yarn Doubling – types, objectives, and application
Doubling reduces unevenness of single yarns and the strength of the doubled yarn is correspondingly better than the single yarns. In this article Ring Doubling, Two-For-One (TFO) twister, quality required by yarn to get best-doubled yarn…
Read More...
Read More...
Automatic cone winding
Specifications of automatic cone winding, checking of reeling frequently, reeling doff weight, reeling calculations
Read More...
Read More...
Yarn Finishing System
Contains the process sequence of Finishing for yarn. It includes yarn twist setting, cone winding from ring cops to cone by cone winding , ordinary cone winding specifications, slub catcher settings , splicing, production calculation.
Read More...
Read More...
Optimum Yarn Spinning conditions
Factors governing Optimum Spinning condition, Yarn quality assessment, Causes of end breakage/ end down
Read More...
Read More...
Lap Former Process
In Lap-former machine, slivers are fed to form a lap of 20 inches wide condensed with a slight draft and weighing as per set length. The machine run smoothly so as not to disturb the fibres which undergo combing at the comber machines. One…
Read More...
Read More...
Speed frame
Objectives of speed frame, operations involved in speed frame
Read More...
Read More...
Combing Machine in Ring Spinning
Necessity of combing, objectives of combing, Combers Noel
Read More...
Read More...
Objectives of carding
Objectives of carding, main actions of carding machine, Useful sliver hanks of different counts and wastage in carding.
Read More...
Read More...