Routine Textile Finishes

Routine finishes are applied to almost all fabrics with an aim to improve their appearance. A finish is anything that is done to a fabric after weaving or knitting, to changes its appearance, hand and performance. When a finish is applied, say on cotton, it might become more shiny, stronger or resist shrinking on washing. Similarly, other finishes may make the fabric softer or stiffer; water or stain resistant; coloured or designed.

Routine Textile Finishes

Scouring/cleaning

Fabrics received as gray cloth have a lot of impurities naturally present in them. These may be oils, waxes and dirty stains acquired during construction of the fabric. Complete removal or cleaning of these impurities is important before applying any other finish. This cleaning is called scouring and is done to all fabrics with the help of soap solutions and chemicals. After cleaning, the fabric becomes smooth, neat and more absorbent

Bleaching

When fabrics are made, they are not white in color, due to impurities and coloring material present in them. To make them white or to dye them in light colors they are bleached. Suitable bleaching agents are used to removing the color from the fabric. Bleaching is done for cotton, woolens and silks. Man-made fabrics do not need bleaching as they are naturally white.

Bleaching has to be done very carefully as the chemical which can destroy the color may also damage the fabric to some extent. Hydrogen peroxide is a universal bleach which can be applied to all kinds of fabrics.

Stiffening

The stiffening means the fabric which is generally limp becomes stiff when a stiffening agent is applied. For stiffening silk, gums are used.
Stiffening gives body, smoothness, and luster to the fabric. This practice is sometimes used to cheat the customer. You must have observed that sometimes if you rub a fabric between your hands, some white powder comes out. It is because the fabric has been over-starched. Interior fabrics are over-starched to look dense and better.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device

The Selvedge · free · one email a week

Know what changed in textiles this week.

Our register tracks 3,130 textile standards. Nobody reads them all, so once a week we tell you which ones moved, and what else is new.

  • Standards added, revised or withdrawn that week
  • One textile calculation, worked through to its answer
  • New and revised guides on the site
  • Textile fairs coming up, with their dates

Free when you confirm: Spinning and Weaving Calculations (PDF). 49 calculations, from the blowroom to the loom, each with its formulas and a worked example.

We send a confirmation link first. Unsubscribe in one click, any time.

  • No spam
  • Your address is not shared
  • Unsubscribe in one click