India's Agro Textiles (Quality Control) Order, 2023 covers 20 products, from insect and hail nets to mulch mats and lay-flat tubes, and has applied since 1 July 2024. Each item's Indian Standard and BIS licence count, where shade nets stand, the tests a licence needs, and a worked hail-net example.

Agro textiles QCO: 20 items need the BIS mark, and shade nets are not one of them. In force since 1 July 2024.

India’s agro textiles QCO is the Agro Textiles (Quality Control) Order, 2023 (S.O. 4248(E), dated 27 September 2023). It names 20 products, each tied to one Indian Standard, and since 1 July 2024 every one of them has had to carry the BIS Standard Mark under a licence, whether it is made in India or imported. Goods made for export are outside it. On 10 October 2026, BIS’s standards portal listed 59 operative licences across the 20 standards, and none for nine of the items, mulch mats among them. Shade nets are not on the list.

This page takes that one order apart: the 20 items grouped by kind, with the licences BIS lists for each; how the start date moved; where shade nets stand; what a hail-net or mulch-mat licence is tested on; and a worked example of what a hail net has to stop. Our technical textiles QCO list sets this order beside the geotextile, protective, medical, rope and industrial ones; what agro-textiles do in the field is in our agrotech overview.

The short version

  • The order. Agro Textiles (Quality Control) Order, 2023, made by the Ministry of Textiles under section 16(1) and (2) of the BIS Act, 2016, read with section 17 and section 25(3).
  • 20 items, 18 standard numbers. Two standards come in two parts: fencing nets (IS 17358) and hail protection nets (IS 17730).
  • In force from 1 July 2024, for every firm. The order first said 1 April 2024; S.O. 1579(E) of 28 March 2024 moved it. There is no later start for micro or small firms, no self-help-group exemption and no window for selling unmarked old stock.
  • The obligation. Each item must conform to its Indian Standard and carry the Standard Mark under a BIS licence granted under Scheme-I of Schedule-II to the BIS (Conformity Assessment) Regulations, 2018. BIS certifies and enforces.
  • Exempt. Goods meant for export. Nothing else.
  • Not in this order. Shade nets (IS 16008), and mulch made of plastic film rather than spunbond nonwoven.

How the start date moved

Notification Dated What it did
S.O. 4248(E), the order 27 Sep 2023 Made the order, to come into force on 1 Apr 2024 (Gazette of India, Extraordinary, No. 4078)
S.O. 1579(E), the Agro Textiles (Quality Control) Amendment Order, 2024 28 Mar 2024 Substituted paragraph 1(2): the order comes into force on 1 Jul 2024. The amendment itself took effect on publication (Gazette No. 1498)

BIS’s list of products under compulsory certification (updated 8 October 2026) names these two notifications and no later one, and its standards portal marks each of the 20 standards “QCO Notified & Implemented”, with 1 July 2024 as the date. All 20, and the shade-net standard, belong to the same BIS committee, TXD 35 (Technical Textiles for Agrotech Applications).

The two texts differ on new editions. The Hindi text of the order ends its schedule with a note that the latest version of each Indian Standard applies from the date BIS publishes it. The English text has no such note. No standard on the list has had a new edition since the order was made (BIS’s portal, 10 October 2026), so the difference has not yet mattered. Amendments have been issued, and are counted in the table below.

Agro textiles QCO: the 20 items, their standards and licences

The first three columns are the order’s own, grouped by kind of product with the order’s item numbers kept. “Amendments” is what BIS lists for the standard. The last column is the number of operative licences BIS’s Know Your Standards portal listed under each standard on 10 October 2026; each standard links to its page there.

Item Product, as the order names it Indian Standard Amendments BIS lists Licences, 10 Oct 2026
Nets (8 items, 29 licences)
2 Insect nets IS 16513:2016 3 (see note) 13
11 Windshield nets IS 17356:2020 None 0
12 Harvest nets IS 17357:2020 None 0
13 Fencing nets (extruded polymer) IS 17358 (Part 1):2020 None 0
14 Fencing nets (monofilament and tape yarn) IS 17358 (Part 2):2020 1 (see note) 0
15 Plant support nets IS 17513:2020 None 1
18 Hail protection nets (knitted) IS 17730 (Part 1):2021 2 (see note) 6
19 Hail protection nets (woven) IS 17730 (Part 2):2021 2 9
Spunbond polypropylene nonwovens (2 items, 1 licence)
1 Crop cover and fruit skirting bags IS 16718:2021 None 1
10 Non-woven mulch mat IS 17355:2020 None 0
Woven and laminated woven covers, beds and tubes (6 items, 28 licences)
3 Woven ground covers for horticulture IS 16202:2014 2 10
5 Vermiculture beds IS 15907:2010 2 10
7 HDPE laminated woven flat lay tube for irrigation IS 16190:2014 3 4
9 HDPE laminated woven flat lay tube for drip irrigation IS 16627:2017 None 1
16 Flat lay tube for rain irrigation system IS 17728:2021 None 0
20 Orchard protection covers IS 17731:2021 1 3
Flexible water storage tank (1 item, 1 licence)
17 Flexible water storage tank IS 17729:2021 None 1
Jute (2 items, no licence)
4 Jute mat IS 17070:2019 None 0
6 Sapling bags IS 16089:2013 1 0
Knitted gloves (1 item, no licence)
8 Nylon knitted seamless gloves IS 16390:2015 None 0

Note on amendments. BIS’s own records disagree for three standards. For IS 16513, the portal’s summary says no amendment, but its list of Gazette notices and BIS’s product manual (April 2025) both count three. For IS 17730 (Part 1), the portal lists two amendments (2021 and 2024) and the product manual of June 2026 says three. IS 17358 (Part 2) appears twice in the portal, once with one amendment and once with none. Ask the BIS branch office for the amendment list before applying for a licence.

Who holds the licences. All 59 are operative and every one is at an Indian address. Gujarat holds 25 of them, Maharashtra 11 and Madhya Pradesh 6. By the scale BIS records, 21 are held by large firms, 23 by medium, 14 by small and 1 by a micro firm. Nets and woven covers, beds and tubes account for 57 of the 59. Nine items have no licence at all: the jute mat, jute sapling bags, nylon gloves for tobacco harvesters, the spunbond mulch mat, windshield nets, harvest nets, both kinds of fencing net and the lay-flat tube for rain irrigation.

Like every item on the list, those nine may not be made, imported or sold in India without the mark (see “What the order requires” below), so a buyer offered a marked mulch mat or harvest net should ask for the licence number and look it up on the portal.

Shade nets are not on the list

Shade nets have their own Indian Standard in two parts: IS 16008 (Part 1):2016, for nets made from tape yarns, and IS 16008 (Part 2):2016, for nets made from monofilament yarns. Neither part is in the order’s schedule, and IS 16008 appears nowhere in BIS’s compulsory-certification list, so no order requires the mark on a shade net.

Many makers hold a licence anyway. On 10 October 2026 the portal listed 14 operative licences under Part 1 and 15 under Part 2: 29 in all, more than under any single standard the agro order names. BIS’s product manual for Part 1 (September 2023) sets the licence scope by shade percentage: Type I at 50%, Type II at 75% and Type III at 90%.

Two things follow for a shade-net maker:

  • A claim needs a licence. Section 17(2) of the Act bars anyone from claiming, in advertising, price lists or on the goods, that a product conforms to an Indian Standard without a valid licence or certificate of conformity from BIS or another authority the government has approved. “IS 16008” printed on an unlicensed roll is such a claim.
  • The next net on the same line may be in the order. Insect nets, windshield nets, harvest nets, fencing nets, plant support nets and hail protection nets all are. At least six firms on the portal’s lists hold both a shade-net licence and a hail-net licence.

A net rated by its shade percentage does not necessarily pass photosynthetically active radiation at that rate; the shade net PAR calculator works out what reaches the crop.

What a hail-net licence is tested on, beside a shade net’s

BIS publishes a product manual for each standard: the tests, which a licensee must run in-house (“R”) and which it may send out (“S”), and how often. The manuals for hail nets, Part 1 (June 2026) and Part 2 (August 2024), ask for most of what the shade-net manuals (Part 1 and Part 2, September 2023) do, plus up to three more. In both, the control unit is a day’s rolls or bundles of one type made to the same parameters.

Test Shade nets (IS 16008) Hail nets (IS 17730) Method the manual cites
Yarn linear density and heat shrinkage at 60 °C and 95 °C Four samples every 8 hours Four samples every 8 hours The standard itself; bought-in yarn can be covered by a test certificate or laboratory report
Mass Each control unit Each control unit IS 1964
Breaking strength, both directions Each control unit Each control unit IS 1969 (Part 1), which BIS pairs with ISO 13934-1
Bursting pressure Each control unit Each control unit IS 1966 (Part 1) or (Part 2), paired with ISO 13938-1 and ISO 13938-2
Shading percentage Each control unit Each control unit The standard’s Annex C, on a shade meter
Breaking strength kept after UV exposure Part 1 every 15 days; Part 2 every six months Every six months (144 hours’ exposure), and on any change of material source The standard’s Annex B
Colour fastness to artificial light, coloured nets only Every six months Every six months IS/ISO 105-B02
Cold cracking resistance Not required Each control unit The standard’s Annex E, on an impact tester
Seam (joint) strength Not required Each control unit IS/ISO 13935-1
Porosity Not required Woven nets (Part 2) only, each control unit The standard’s Annex D

The frequencies are BIS’s recommended levels of control; a licensee may propose its own in its quality plan. The laboratory rules have loosened in the newer manuals. The June 2026 manual for knitted hail nets says there is no obligation to keep an in-house laboratory: a shared or cluster facility, a BIS-recognised or empanelled laboratory, or one accredited to ISO/IEC 17025 will do. The 2024 manual for woven hail nets makes the in-house laboratory optional for MSMEs. The 2023 shade-net and mulch-mat manuals still say a laboratory shall be maintained. A factory outside India applies under BIS’s Foreign Manufacturers Certification Scheme, whose page says it must have the equipment and competent staff to test the product on its own premises, and must file a separate application for each standard and each factory.

Worked example: what a hail net has to stop

None of the tests above grades a net by the hailstone it will stop; that depends on the canopy as much as on the net. The hail net impact calculator works out the energy of a falling stone and what the net and its cables feel when they stop it. Take a canopy designed for a 30 mm stone, with the calculator’s own defaults: ice at 900 kg/m³, a drag coefficient of 0.5, air at 1.225 kg/m³, 150 mm of net deflection on impact, 4 m between supports and 120 stones per square metre. Then run a 20 mm and a 40 mm stone through the same canopy, and the 30 mm stone through a tighter net. Each row opens the calculator with its inputs.

Design stone Stone mass Falling speed Energy per stone Peak force on the net Cable tension Storm energy per square metre
20 mm 3.77 g 19.61 m/s 0.72 J 9.66 N 64.41 N 86.95 J/m²
30 mm 12.72 g 24.01 m/s 3.67 J 48.91 N 326.05 N 440.17 J/m²
40 mm 30.16 g 27.73 m/s 11.59 J 154.57 N 1,030.49 N 1,391.16 J/m²
30 mm, net deflecting 75 mm 12.72 g 24.01 m/s 3.67 J 97.82 N 1,304.21 N 440.17 J/m²
  • Energy rises with the fourth power of the diameter. Falling speed grows with the square root of the diameter and mass with its cube, so doubling the stone from 20 mm to 40 mm multiplies the energy by 16, from 0.72 J to 11.59 J. Going from 30 mm to 40 mm multiplies it by 3.16.
  • A tighter net is not a stronger canopy. Halve the deflection from 150 mm to 75 mm and the peak force on the net doubles, to 97.82 N, while the tension in the support cable quadruples, to 1,304.21 N.
  • The cable carries more than the net. At 30 mm the cable tension is 326.05 N against a peak force of 48.91 N, because the 4 m span levers the load.

For a hail-net maker, the BIS mark shows the net meets IS 17730 on strength, bursting, UV durability, cold cracking and seams. A claim such as “protects against hail up to 30 mm” is a different promise, and it holds only for a stated canopy: give the design stone, the deflection and the span behind it. The calculator’s model is deliberately simple: a smooth sphere at a steady speed in still air, and a net that stretches linearly. Real stones can arrive faster and real peaks run higher, and the support structure needs an engineer’s sign-off.

The mulch mat on the list, and the one that is not

Item 10 is a non-woven mulch mat to IS 17355:2020, a polypropylene spunbonded mat for agricultural and horticultural use. Item 1, crop covers and fruit skirting bags to IS 16718:2021, is the same kind of spunbond fabric. On 10 October 2026 BIS’s portal listed no licence under IS 17355 and one under IS 16718. How spunbond is made is covered in our non-woven fabrics guide.

A mulch film is a different product. A polyethylene or biodegradable film is not a spunbond nonwoven, and it is not one of the 20 items. BIS’s product manual for IS 17355 (April 2023) sets out what a mat licence is tested on:

Test Method How often, per the manual
Length and width IS 1954 In-process controls
Mass per unit area IS 15891 (Part 1), paired with ISO 9073-1 Each control unit
Thickness IS 15891 (Part 2) In-process controls
Tensile strength and elongation, machine and cross direction IS 15891 (Part 3), paired with ISO 9073-3 Each control unit
Trapezoid tear strength, both directions IS 15891 (Part 4), paired with ISO 9073-4 Each control unit
Colour Visual, against the standard Each control unit
Ash content The standard’s Annex C Once a week
UV stability The standard’s Annex B; may be sent to a laboratory Once a month

The control unit is a day’s rolls made under similar conditions from the same raw material; the licence sample is 10 m of mat, and the licence covers Type 1 or Type 2. Every test except UV stability is marked “R”, to be run in-house.

What the order requires, and of whom

  • Everyone who handles the goods. Under section 17(1) of the BIS Act, 2016, nobody may make, import, distribute, sell, hire, lease, store or display for sale an item the order covers without the Standard Mark under a valid licence.
  • Exports. Goods meant for export are outside the order (paragraph 2).
  • Who certifies. BIS is the certifying and enforcing authority (paragraph 4). No other body is named.
  • Penalties. Paragraph 5 makes any contravention punishable under the BIS Act, 2016; section 29 of the Act sets the penalties (BIS's copy of the Act).

How this page is kept

Last verified: 10 October 2026. The order and its amendment are read from the Gazette of India, both linked where they are used; the list of notifications from BIS’s compulsory-certification list (updated 8 October 2026); editions, amendments and licence counts from BIS’s Know Your Standards portal on 10 October 2026; the tests from BIS’s product manuals for IS 17355, IS 17730 (Parts 1 and 2) and IS 16008 (Parts 1 and 2); the foreign-factory conditions from BIS’s scheme page (updated 23 December 2025); and sections 17 and 29 from BIS’s copy of the BIS Act, 2016. The hail figures were computed with the calculator’s own formula and checked on its page through the links above. Licence counts change daily, so check a supplier on the portal itself. This page describes what the instruments say; it is not legal advice for a particular product or shipment. Corrections are welcome through the contact page.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device

The Selvedge · free · one email a week

Know what changed in textiles this week.

Our register tracks 3,130 textile standards. Nobody reads them all, so once a week we tell you which ones moved, and what else is new.

  • Standards added, revised or withdrawn that week
  • One textile calculation, worked through to its answer
  • New and revised guides on the site
  • Textile fairs coming up, with their dates

Free when you confirm: Spinning and Weaving Calculations (PDF). 49 calculations, from the blowroom to the loom, each with its formulas and a worked example.

We send a confirmation link first. Unsubscribe in one click, any time.

  • No spam
  • Your address is not shared