Importance of Air Permeability/Fabric porous structure in production of technical textile fabrics

Fabric air permeability is a measure to what extent it gives air passing through the fabric. The porosity of fabric is the demonstration of the air gap as a percentage within the fabric. It has been important for especially the tent fabric and parachute.

Importance of Air Permeability/Fabric porous structure in production of technical textile fabrics Read More »

water-repellent-leaf

Introduction to breathable water-repellent textiles and their production methods

Breathability refers to the ability of a fabric to absorb moisture and release it through the material itself, allowing it to ‘breathe’. Breathable Fabrics transmit body moisture away from the body, thus maximizing comfort and dryness during outdoor activities.

Introduction to breathable water-repellent textiles and their production methods Read More »