Jump to a calculator 671 tools
Wet Processing
Liquor Ratio (MLR) & Water Consumption Calculator
The dye bath is rarely the problem. Rinses are where the water bill is made.
Dye Bath Volume
— L
Batch weight multiplied by the liquor ratio
Water Account
- Total Water per Batch
- — m3
- Water per kg of Fabric
- — L/kg
- Water Cost per Batch
- —
- Water Cost per kg
- —
Dropping from 1:10 to 1:6 cuts water, salt, steam and effluent together. It is the single highest-leverage change in an exhaust dyehouse.
Using this calculator
About the Liquor Ratio (MLR) & Water Consumption Calculator
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
liquorVolume = fabricWeight x liquorRatioA liquor ratio of 1:8 means eight litres of bath for every kilogram of goods. Every chemical dosed in grams per litre is therefore dosed against this number, not against the fabric.
totalLitres = liquorVolume x (1 + rinses)The dye bath is one fill. Each rinse is another one of the same size, which is why rinse count matters as much as the ratio itself.
waterPerKg = totalLitres / fabricWeight batchWaterCost = totalLitres / 1000 x waterCostLitres per kilogram is the benchmarking unit the whole industry reports in, and the only one that compares a 500 kg jet against a 2,000 kg one honestly.
| Symbol | Stands for | Unit |
|---|---|---|
fabricWeight | Fabric Batch Weight | kg |
liquorRatio | Liquor Ratio (1 : x) | :1 |
rinses | Rinse Fills after Dyeing | no. |
waterCost | Water Cost | /m3 |
liquorVolume | Dye Bath Volume | L |
totalWater | Total Water per Batch | m3 |
waterPerKg | Water per kg of Fabric | L/kg |
batchWaterCost | Water Cost per Batch | — |
costPerKg | Water Cost per kg | — |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The batch weight and the machine liquor ratio fix the bath volume.
- Each rinse fill is counted as a further bath of the same volume — a simplification that is close to true on a jet and conservative on a winch.
- Total volume is converted to cubic metres and priced.
- Water per kilogram is reported separately, because that is the figure a sustainability report and a machine purchase decision both turn on.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Fabric Batch Weight | kg | 1 to 100000 kg | 500 | |
| Liquor Ratio (1 : x) | :1 | 1 to 50 :1 | 8 | |
| Rinse Fills after Dyeing | no. | 0 to 20 no. | 5 | |
| Water Cost | /m3 | 0 to 100 /m3 | 0.5 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Dye Bath Volume (headline result) | L | Batch weight multiplied by the liquor ratio |
| Total Water per Batch | m3 | |
| Water per kg of Fabric | L/kg | |
| Water Cost per Batch | — | |
| Water Cost per kg | — |
Worked example
Given
- Fabric batch weight
- 500 kg
- Liquor ratio
- 1:8
- Rinse fills
- 5
- Water cost
- 0.50 per m3
Substituting
bath = 500 x 8 = 4,000 Lfills = 1 + 5 = 6total = 4,000 x 6 = 24,000 L = 24 m3per kg = 24,000 / 500 = 48 L/kgAnswer
- Dye bath volume
- 4,000 L
- Total water
- 24.00 m3
- Water per kg
- 48.00 L/kg
- Batch water cost
- 12.00
- Cost per kg
- 0.024
Move the same batch to a 1:5 machine and total water falls to 15 m3 — a 37% cut, before counting the salt, the steam to heat it and the effluent that follows it.
How to use it
- Work through the input groups in order — Batch and Process. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Dye Bath Volume in the dark results panel — that is the headline figure, expressed in L.
- Check the supporting rows underneath (Total Water per Batch, Water per kg of Fabric, Water Cost per Batch and Water Cost per kg) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Water and effluent budgeting for a dyehouse, batch by batch or programme by programme.
- Machine selection — justifying a low liquor ratio machine on water, salt, steam and effluent together rather than on water alone.
- Recipe dosing — chemicals specified in grams per litre have to be multiplied by the bath volume this tool gives.
- Sustainability reporting — litres per kilogram is the unit most buyer scorecards and benchmarks are written in.
Reading the result
Typical bands and what each one is telling you.
| Value | What it indicates |
|---|---|
| Under 30 L/kg | Modern low liquor jet with controlled rinsing. Best practice for exhaust dyeing. |
| 30 to 60 L/kg | Typical of a well-run conventional dyehouse. The example sits here. |
| 60 to 100 L/kg | High. Usually too many rinse fills rather than too high a ratio — count them before blaming the machine. |
| Above 100 L/kg | Winch or jigger practice with uncontrolled overflow rinsing. The largest single saving available in most dyehouses. |
Assumptions and limits
- Dropping from 1:10 to 1:6 cuts water, salt, steam and effluent together. It is the single highest-leverage change in an exhaust dyehouse.
- Every input is bounded to the range normal practice occupies (Fabric Batch Weight 1 to 100000 kg, Liquor Ratio (1 : x) 1 to 50 :1 and Rinse Fills after Dyeing 0 to 20 no., and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Standards and further reading
- ZDHC and Higg FEM report water use per kilogram of production, which is the waterPerKg output.
- IPPC BAT reference document for the textiles industry — benchmark specific water consumption figures by process.
On this site
Articles that explain what this tool calculates.
Questions people ask
Does a lower liquor ratio save chemicals as well as water?
Salt and auxiliaries, yes — they are dosed in grams per litre, so halving the bath halves the quantity. Dyestuff is dosed on the weight of fabric, so it does not change, but the lower volume raises exhaustion and can allow a small reduction. Steam falls with volume too, since there is less water to heat.
What counts as a rinse fill?
Any complete fill and drain at the machine liquor ratio. Continuous overflow rinsing is harder to count — estimate it as the total volume passed through divided by the bath volume, and it is usually a larger number than anybody expects.
Is the machine rated ratio the ratio I actually get?
Rarely, at part load. A jet rated 1:5 at full load runs a higher effective ratio on a short batch, because the minimum bath the pump and nozzle need does not shrink with the load. Enter the effective ratio for the batch size being run, not the nameplate figure.
Convert this result
Reference rate of 2026-11-16, published by the European Central Bank. Source
A reference rate is not a dealing rate. Banks and payment providers apply their own spread, so treat this as the mid-market figure a quotation is negotiated around rather than the money that will arrive.