Focus on cotton, wool, silk, flax, hemp, jute, and regional fibers. Agronomy, harvesting, ginning, scouring, and lifecycle impacts. This section explains practical decision criteria, typical test methods, and failure modes that matter in real production. Readers get checklists, calculation steps, and case examples connecting specifications to cost, reliability, and compliance. Links map core concepts to upstream inputs and downstream processes so choices remain consistent across sourcing, manufacturing, and end-use performance. Each article includes definitions, diagrams where helpful, and plain-language notes to help newcomers ramp quickly while giving experienced professionals the depth needed to troubleshoot and optimize. Standards references are cited with context, and whenever trade-offs exist, we make them explicit so you can defend decisions.

ring-spinning-machine

Optimum Drafting Conditions of Polyester and Viscose Blend Yarns

In this study, we used an experimental design to investigate the influence of the total draft, break draft, the distance between the aprons (Clips) and production roller pressure on yarn quality in order to obtain optimum drafting conditions for polyester and viscose (PES/CV) blend yarns in ring spinning frame. We used PES fibres (1.4 dtex × 38 mm long) and CV fibres (1.6 dtex × 38 mm long) to spin a 20 Tex blend yarn of PES (70%)/CV (30%) blend ratio.

When the break draft, adjustment of distance between of aprons and roller pressure is not reasonable, controlling and leading of the fibres is not sufficient for proper orientation of the fibres in the yarn structure to produce a high-quality yarn. Experimental results and statistical analysis show that the best yarn quality will be obtained under drafting conditions total draft of 38, 1.2 break draft, 2.8 mm distance between of aprons and maximum pressure of the production top roller (18daN).

Read more »

Article

Scroll to Top