Home » Machinery specifications » Hans Schmidt ZF2 / ZD2

Hans Schmidt ZF2 / ZD2

Checked by an editor

Mechanical hand-held tension meters with an analogue dial for measuring low tensions of fibres, threads and fine wires. The material is threaded over three V-shaped, ball-bearing guide rollers. The ZF2 measures up to 100 cN with small guide rollers (groove Ø 7.4 mm) for tight spaces and is the model most used in circular knitting; the ZD2 measures up to 300 cN with guide rollers of groove Ø 12 mm for the textile and wire industries.

Yarn testingTesting and laboratoryIn the builder's current range

Key specifications

Specifications incomplete: 0 of 5 key figures recorded

  • Yarn test speed (evenness / hairiness)—
  • Force capacity—
  • Tensile (crosshead) speed—
  • Yarn count range—
  • Test standards—
See it
Exhibited at ITMA ASIA + CITME 2024, Shanghai, stand H8-A04 (as listed by the organiser)

Specification

ParameterValueUnit
ZF2 measuring ranges available7
ZF2 measuring range span1 - 5 cN bis 10 - 100cN
ZF2-5 measuring range1 – 5cN
ZF2-10 measuring range1 – 10cN
ZF2-12 measuring range1 – 12cN
ZF2-20 measuring range2 – 20cN
ZF2-30 measuring range3 – 30cN
ZF2-50 measuring range5 – 50cN
ZF2-100 measuring range10 – 100cN
ZF2 measuring head width43mm
ZF2 accuracy±1 % Vollausschlag (Full Scale) oder ±1 Skalenteilstrich
ZF2 scale diameter54mm
ZF2 temperature range10 – 45ºC
ZF2 air humiditymax. 85% rel. Feuchte
ZF2 housing materialPlastic (POM)
ZF2 weight, net (gross)ca. 200 (600)g
ZF2 max. throughput speed, guide rollers Standard900m/min
ZF2 max. throughput speed, guide rollers Code K2000m/min
ZF2 max. throughput speed, guide rollers Code T450m/min
ZF2 max. throughput speed, guide rollers Code W450m/min
ZD2 measuring ranges available6
ZD2 measuring range span3 - 30 cN bis 20 - 300cN
ZD2-30 measuring range3 – 30cN
ZD2-50 measuring range5 – 50cN
ZD2-100 measuring range10 – 100cN
ZD2-150 measuring range20 – 150cN
ZD2-200 measuring range20 – 200cN
ZD2-300 measuring range20 – 300cN
ZD2 measuring head width63mm
ZD2 accuracy±1% Vollausschlag (Full Scale) oder ±1 Skalenteilstrich
ZD2 scale diameter54mm
ZD2 temperature range10 – 45ºC
ZD2 air humiditymax. 85% rel. Feuchte
ZD2 housing materialPlastic (POM)
ZD2 weight, net (gross)ca. 220 (620)g
ZD2 max. throughput speed, guide rollers Standard2000m/min
ZD2 max. throughput speed, guide rollers Code K3500m/min
ZD2 max. throughput speed, guide rollers Code H5000m/min
ZD2 max. throughput speed, guide rollers Code T1000m/min
ZD2 max. throughput speed, guide rollers Code W1000m/min
ZD2 max. throughput speed, guide rollers Code ST1000m/min
ZD2 max. throughput speed, guide rollers Code CE21000m/min
ZF2 guide roller groove diameter7.4mm
ZD2 guide roller groove diameter12mm

Read from the builder's published page: www.hans-schmidt.com, on 2026-11-07.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.hans-schmidt.com,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device