The TWF-NCR random card processes cotton, natural fibers, and man-made fibers into bulky, soft random webs. It features dynamic web formation via tambour, doffer, and air guide plate, which enables an excellent machine direction (MD) and cross direction (CD) strength ratio with reduced nep formation.

Nonwoven cardingNonwovensIn the builder's current range

Specification

ParameterValueUnitComparable
Throughput (max.)< 260kg/h
Working width≤ 3,800mm
Fiber fineness0.7–17dtex0.07–1.7 tex
Fiber length14–60mm
Web weight25–140gsm

Read from the builder's published page: www.truetzschler.com, on 2026-11-12.

Standards that apply to this class

Machines of this class fall under the textile machinery standards for nonwoven machinery. The common requirements of ISO 11111-1 apply to every machine in this family.

Safety
ISO 11111-3 Textile machinery — Safety requirements — Part 3: Nonwoven machinery — Amendment 2
Noise
ISO 9902-3 Textile machinery — Noise test code — Part 3: Nonwoven machinery — Amendment 1

These standards cover the class of machine, not this model. A machine's own declaration of conformity says which editions it was built to.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.truetzschler.com,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device