Hemp belongs to the Angiosperm phylum since it has vessel elements in the woody core (xylem) like hardwood.

hemp plants

Hemp belongs to the Angiosperm phylum since it has vessel elements in the woody core (xylem) like hardwood. It belongs to the eudicotyledons like hardwoods, numerous bushes, and herbs since it has two cotyledons (i.e. seed leaves).

The long and flexible hemp fibers are embedded in the bark (cortex) on
the surface of the stem. Hemp originates from Central Asia but can be cultivated from the Equator to the polar circle.

Hemp Fiber

One of the reasons hemp fiber has been valued is because of its length. The primary bast fibers in the bark are 5–40 mm long, and are amalgamated in fiber bundles which can be 1–5 m long (secondary bast fibers are about 2 mm long). The woody core fibers are short—about 0.55 mm—and like hardwood fibers are cemented together with considerable lignin.

The core fibers are generally considered too short for high-grade paper applications (a length of 3 mm is considered ideal), and too much lignin is present. While the long bast fibers have been used to make paper almost for 2 millennia, the woody core fibers have rarely been so used.

Other desirable features of hemp fibers are strength and durability (particular resistance to decay), which made hemp useful in the past for rope, nets, sail-cloth, and oakum for caulking. During the age of sailing ships, Cannabis was considered to provide the very best of canvas, and indeed this word is derived from Cannabis.

The hemp fibers are present in bundles as long as the stems, which can easily be peeled off the xylem surface by hand or machine. The fresh stem consists of a hollow cylinder of 1-5 mm thick xylem covered by 10-50 µm cambium, 100-300 µm cortex, 20-100 µm epidermis and 2-5 µm cuticle. The pith is empty space in dry stems.

Hemp Plant

help plant

Highly selected forms of the fiber cultigen possess features maximizing fiber production. Since the nodes tend to disrupt the length of the fiber bundles, thereby limiting quality, tall, relatively unbranched plants with long internodes have been selected.

Another strategy has been to select stems that are hollow at the internodes, with limited wood, since this maximizes production of fiber in relation to supporting woody tissues.

Similarly, limited seed productivity concentrates the plant’s energy into production of fiber, and fiber cultivars often have a low genetic propensity for seed output. Selecting monoecious strains overcomes the problem of differential maturation times and quality of male (staminate) and female (pistillate) plants (males mature 1–3 weeks earlier).

Male plants, in general, are taller, albeit slimmer, less robust, and less productive. Except for the troublesome characteristic of dying after anthesis, male traits are favored for fiber production, in contrast to the situation for drug strains noted below. In former, labor-intensive times, the male plants were harvested
earlier than the females, to produce superior fiber.

The limited branching of fiber cultivars is often compensated for by possession of large leaves with wide leaflets, which obviously increase the photosynthetic ability of the plants. Since fiber plants have not generally been selected for narcotic purposes, the level of intoxicating constituents is usually limited.

Typical architecture of categories of cultivated Cannabis sativa. Narcotic plants are generally low, highly branched, and grown well-spaced. Plants were grown for oilseed was traditionally well-spaced, and the plants developed medium height and strong branching.

Fiber cultivars are grown at high density and are unbranched and very tall. “Dual purpose” plants are grown at moderate density, tend to be slightly branched and of medium to tall height. Some recent oilseed cultivars are grown at a moderate density and are short and relatively unbranched.

The degree of branching and height are determined both by the density of the plants and their genetic background.

Fiber Processing

hemp fiber

Unlike flax, hemp long fiber requires water retting for preparation of high-quality spinnable fibers for production of fine textiles. Improved microorganisms or enzymes could augment or replace traditional water retting. Steam explosion is another potential technology that has been experimentally applied to hemp.

The traditional procedure for the production of fibers from hemp is field retting, a natural process which results in fibers of variable quality due to differences in weather conditions. During this process fungi and yeasts colonize the hemp and produce polysaccharide-degrading enzymes, which macerate and disrupt
the parenchyma cells. This process can be replaced with the more controllable water retting procedure in which the plant stems are placed in tanks with 30-40°C hot water for 4 days.

After retting, the woody core is broken into small pieces that can be separated from the fibers by decortication. This is industrially done with pairs of rotating rollers, which crush the shives. In lab-scale, the fibres are isolated with hand peeling. The extracted fibres are in the form of large fibre bundles useful in non-woven fibre mats, which are made by air-drying and needle punching with uncontrolled and thereby random fiber orientation. Production of aligned fiber assemblies can also be done at laboratory scale by combing the fibers in water, stretching them and air-drying them.

Defibration

During water retting, the hemp bast is separated into large fiber bundles. Additional treatment is required to defibrate the fiber bundles into single fibers and small fiber bundles useful for production of hemp yarn. It is done by degradation or disruption of the middle lamellae between the single fibres.

Enzyme treatment, wet oxidation and NaOH treatment can degrade pectin and lignin in the middle lamellae between the single fibres.

Yarn Formation

The retted fibre bundles of 0.5-2 m length are traditionally used directly for production of yarn for rope production. First hackling is done in two steps to straighten the fibers and remove short disordered fibers with a metal-pinned brush; this results in a sliver of parallel fibers useful for spinning.

At the industrial scale, the hackling is performed using metal-pinned brushes and rotating rollers to pull the fibres forward. This technique is basically also used to make sliver of shorter fibres like flax fibres.

By manual yarn spinning, some fibres from the sliver are mounted on a rotating hook. The fibres are stretched during the twisting process and more fibres are added, while the hand is moved backward to elongate the spun amount of yarn and keep a constant yarn thickness.

At industrial scale, the stretching part of this process is called drafting. In drafting, the fibres become straightened by passing the sliver through a series of rollers with increasing rotational speed in the forward direction.

The drafting process elongates the thick sections of the filament so they get the same thickness as the thinner sections, resulting in a uniform sliver ready for spinning.

The most common spinning method is ring spinning, in which slivers delivered from the drafting rollers become twisted by the traveller that is freely rotating on a ring. The ring distributes the yarn onto a rotating bobbin. Each traveller rotation introduces one twist. Increased delivering speed from the drafting rollers decreases the number of twists per length.

The twisting forces the fibers to take a helical structure and results in inherent sliding friction between the fibers and in axial strength in the yarn. The produced yarn can be wound on a metal frame to get aligned fiber assemblies, ready for composite production.

Hemp Product Usages

Hemp product usages

Hemp paper is useful for specialty applications such as currency and cigarette papers where strength is needed. The bast fiber is of greatest interest to the pulp and paper industry because of its superior strength
properties compared to wood. However, the short, bulky fibers found in the inner part of the plant (hurds) can also be used to make cheaper grades of paper, apparently without greatly affecting quality of the printing
surface. Hemp is not competitive for newsprint, books, writing papers, and general paper (grocery bags, cof-
fee cups, napkins), although there is a specialty or novelty market for those specifically wishing to support the hemp industry by purchasing hemp writing or printing paper despite the premium price.

  • Specialty pulp (cigarette paper, bank notes, technical filters, and hygiene products)
  • Composites for autos
  • Construction & thermal insulation materials
  • Geotextiles
  • Fiberboard
  • Cement (Concrete) and Plaster

The Full Processing Workflow

To see how these mechanical steps connect in modern textile manufacturing, this video overview walks through the full pipeline of turning raw hemp stalks into usable fiber:

3 comments

  1. In the section under Fiber Processing this paper states, “After retting, the woody core is broken into small pieces that can be separated from the fibers by decertification. ”
    This is not correct, the correct word is- decortication.

    1. Textile School Author

      Thank you so much for catching that! We have updated the article with the correct term. We really appreciate you helping us keep the information accurate.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top