Natural Cellulosic Seed Fibres

Cellulose is the substance that makes up most of a plant's cell walls. Since it is made by all plants, it is probably the most abundant organic compound on Earth.Many varieties of plant fibers exist such as hairs (cotton, kapok), fiber-sheafs of dicoltylic plants or vessel-sheafs of monocotylic plants (e.g. flax, hemp, jute, and ramie), and hard fibers (sisal, henequen, and coir), not to mention a large number of fibers obtained from trees.

Major Seed/Fruit-hair fibers

cotton plant

Cotton Fiber

Cotton is a soft, staple fiber that grows in a form known as a boll around the seeds of the cotton plant, a shrub native to tropical and subtropical regions around the world, including the Americas, India, and Africa. The fiber most often is spun into yarn or thread and used to make a soft, breathable textile, which is the most widely used natural-fiber cloth in clothing today. The English name derives from an Arabic word which began to be used circa 1400.

Each cotton fiber is composed of concentric layers. The cuticle layer on the fiber itself is separable from the fiber and consists of wax and pectin materials.

coconut husk

Coir Fiber

This fiber, obtained from husks of the fruit of the coconut palm, Cocos nucifera (palm family, Arecaceae), is mainly produced in India and
Sri Lanka. The fruits are broken by hand or machine, and the fiber extracted from the broken husks from which the coconut has been removed for the copra. The husks are retted in rivers, and the fiber separated by hand beating with sticks or by a decortication machine. The fibers are washed, dried, and hackled, and used in upholstery, cordage, fabrics, mats, and brushes.

kapok tree with fruit

Kapok Fiber

Kapok fiber is obtained from the seed pods of the kapok tree, Ceiba pentandra, of the Kapok tree family (Bombacaceae) which is indigenous
to Africa and southeast Asia; the fiber is produced mainly in Java. The tree
grows to a height of 35 m. The seeds are contained in capsules or pods that are picked and broken open with mallets.

The fioss is dried and the fiber is separated by hand or mechanically. A nondrying oil is produced from the seeds with properties similar to cottonseed oil. The fiber is exceedingly light, with a circular cross-section, thin walls, and a wide lumen. Kapok fibers are moisture resistant, buoyant, resilient, soft, and brittle, but not suitable for spinning.

The traditional uses were in life jackets, sleeping bags, insulation, and upholstery; however, synthetics have replaced most of the applications as filling material and now kapok is mainly used for life preservers. Kapok-filled life preservers can support up to three times the weight of the preserver and do not become waterlogged.

Seed/Fruit-hair Fibers

seed fibers

The seeds and fruits of plants are often attached to hairs or fibers or encased in a husk that may be fibrous. These fibers are cellulosic based and of commercial importance, especially cotton,
the most important natural textile fiber.

2 comments

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device