Textile Unit Converter: Fabric Weight, Tenacity & Yarn Length
Grams per denier and centinewtons per tex differ by 8.826, not by 9.
Fabric Weight
— oz/yd2
The imperial equivalent of the stated GSM
Every Equivalent Unit
- Weight per Linear Metre
- — g/m
- Weight per Linear Yard
- — oz/yd
- Tenacity
- — g/den
- True Stress at Break
- — MPa
- Breaking Length
- — km
- Breaking Force at this Count
- — N
- Yarn Length
- — m/kg
- Yarn Length
- — yd/lb
Every constant here is exact by definition rather than measured: the international yard is exactly 0.9144 m and the avoirdupois pound exactly 0.45359237 kg, so the conversions carry no experimental uncertainty of their own. What they do carry is the uncertainty of the input - a GSM taken from a single 100 cm2 cutter on a fabric with 3% weight variation is precise to four figures and accurate to two. The true-stress figure assumes a solid circular cross-section at the stated density and is meaningful for melt-spun filament; for a staple yarn it is a nominal value only, because a spun yarn has air in it and no single cross-sectional area exists. Yarn count conversion between Ne, Nm, tex and denier lives in the dedicated count converter rather than here.
Using this calculator
About the Textile Unit Converter: Fabric Weight, Tenacity & Yarn Length
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
ozPerSquareYard = fabricGsm / 33.905747One ounce per square yard is 28.349523 g spread over 0.83612736 m2, and the ratio of those two numbers is 33.905747 g/m2. The constant is exact, not rounded: both the ounce and the yard are defined exactly in metric units.
gramsPerLinearMetre = fabricGsm x fabricWidth / 100 ozPerLinearYard = gramsPerLinearMetre x 0.9144 / 28.349523Linear weight is the figure a roll is actually costed and freighted on, and it is the one that changes when the finished width moves without the construction changing.
tenacityGpd = tenacityCnTex / 8.825985Denier is nine times tex, so a strength per denier is nine times a strength per tex - but the numerator is gram-force in one and centinewton in the other, and one gram-force is 0.980665 cN. The full factor is 9 x 0.980665 = 8.825985. Using 9 introduces a 2% error that looks like normal test scatter.
specificStressMpa = tenacityCnTex x fibreDensity x 10 breakingLengthKm = tenacityCnTex / 0.980665Specific stress divides force by mass per unit length; true stress divides it by cross-sectional area. Density is what converts one into the other, which is why a polypropylene yarn and a polyester yarn of equal tenacity are not equally strong in megapascals. Breaking length is the length of yarn whose own weight would break it, and it needs no density at all.
| Symbol | Stands for | Unit |
|---|---|---|
GSM | Fabric mass per unit area | g/m2 |
tex | Mass in grams of 1000 m of yarn | g/1000 m |
den | Mass in grams of 9000 m of yarn | g/9000 m |
rho | Fibre density, mass per unit true volume | g/cm3 |
Lb | Breaking length, the self-supporting length of the yarn | km |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The 5 inputs are read from the form on every keystroke: Fabric Weight, Finished Width, Tenacity, Yarn Linear Density and Fibre Density.
- Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
- The validated values are substituted into the expression above, which resolves Fabric Weight together with every supporting figure in one pass — no value is carried over from a previous entry.
- The supporting outputs — Weight per Linear Metre, Weight per Linear Yard, Tenacity, True Stress at Break, Breaking Length, Breaking Force at this Count, Yarn Length and Yarn Length — come from the same pass, so they always describe the same case as the headline figure.
- Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Fabric Weight | g/m2 | 5 to 2000 g/m2 | 180 | |
| Finished Width | cm | 5 to 600 cm | 150 | |
| Tenacity | cN/tex | 1 to 400 cN/tex | 45 | |
| Yarn Linear Density | tex | 0.5 to 5000 tex | 29.5 | 29.5 tex is Ne 20 |
| Fibre Density | g/cm3 | 0.7 to 3 g/cm3 | 1.38 | PET 1.38, cotton 1.54, nylon 6.6 1.14, PP 0.91 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Fabric Weight (headline result) | oz/yd2 | The imperial equivalent of the stated GSM |
| Weight per Linear Metre | g/m | |
| Weight per Linear Yard | oz/yd | |
| Tenacity | g/den | |
| True Stress at Break | MPa | |
| Breaking Length | km | |
| Breaking Force at this Count | N | |
| Yarn Length | m/kg | |
| Yarn Length | yd/lb |
Worked example
Given
- 0
- 180 g/m2 fabric finished at 150 cm
- 1
- Yarn of 29.5 tex at 45 cN/tex tenacity
- 2
- Polyester fibre density 1.38 g/cm3
Substituting
180 / 33.905747 = 5.3088 oz/yd2180 x 1.50 = 270 g/m, and 270 x 0.9144 / 28.349523 = 8.7087 oz/yd45 / 8.825985 = 5.0986 g/den45 x 1.38 x 10 = 621 MPa; 45 x 29.5 / 100 = 13.275 N1,000,000 / 29.5 = 33,898 m/kgAnswer
- 0
- 5.3088 oz/yd2 and 270 g per linear metre
- 1
- 8.7087 oz per linear yard
- 2
- Tenacity 5.0986 g/den, true stress 621 MPa
- 3
- Breaking length 45.887 km, breaking force 13.275 N
- 4
- 33,898 m/kg, which is 16,815 yd/lb
The yd/lb figure is the check worth knowing: 29.5 tex is Ne 20.02, and Ne x 840 gives 16,817 yd/lb against the 16,815 computed here. The two routes agree to one part in ten thousand, which is the whole chain of constants verifying itself.
How to use it
- Work through the input groups in order — Fabric Weight and Yarn & Tenacity. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Fabric Weight in the dark results panel — that is the headline figure, expressed in oz/yd2.
- Check the supporting rows underneath (Weight per Linear Metre, Weight per Linear Yard, Tenacity, True Stress at Break, Breaking Length, Breaking Force at this Count, Yarn Length and Yarn Length) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Process planning — establishing Fabric Weight before a trial is booked, so machine time and material in Textile Testing & Quality Control are committed against a calculated figure rather than an estimate.
- Costing and quotation — Fabric Weight is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
- Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Fabric Weight) shows how much of the gap in Fabric Weight each variable explains.
- Teaching and study — the accepted ranges bracket normal Textile Testing & Quality Control practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.
Reading the result
Typical bands and what each one is telling you.
| Value | What it indicates |
|---|---|
| 100 - 150 g/m2 | Shirting and light apparel wovens, roughly 3 to 4.4 oz/yd2. |
| 340 - 475 g/m2 | Denim, 10 to 14 oz/yd2 - the range the trade names its fabrics by. |
| 15 - 25 cN/tex | Carded cotton ring yarn. Below 12 cN/tex expect weaving trouble. |
| 60 - 85 cN/tex | High-tenacity polyester and nylon industrial yarn. |
| 200 - 280 cN/tex | Aramid and UHMWPE. Note that UHMWPE reaches this at 0.97 g/cm3, so its MPa figure is far lower than its tenacity suggests. |
Assumptions and limits
- Every constant here is exact by definition rather than measured: the international yard is exactly 0.9144 m and the avoirdupois pound exactly 0.45359237 kg, so the conversions carry no experimental uncertainty of their own. What they do carry is the uncertainty of the input - a GSM taken from a single 100 cm2 cutter on a fabric with 3% weight variation is precise to four figures and accurate to two. The true-stress figure assumes a solid circular cross-section at the stated density and is meaningful for melt-spun filament; for a staple yarn it is a nominal value only, because a spun yarn has air in it and no single cross-sectional area exists. Yarn count conversion between Ne, Nm, tex and denier lives in the dedicated count converter rather than here.
- Every input is bounded to the range normal practice occupies (Fabric Weight 5 to 2000 g/m2, Finished Width 5 to 600 cm and Tenacity 1 to 400 cN/tex, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Standards and further reading
- ISO 1144 - Textiles, Universal system for designating linear density (the tex system).
- ASTM D2256 - Tensile Properties of Yarns by the Single-Strand Method, which defines tenacity as breaking force divided by linear density.
- ISO 3801 / ASTM D3776 - Mass per unit area and mass per unit length of fabric.
- ISO 2060 - Determination of linear density of yarn by the skein method.
On this site
Articles that explain what this tool calculates.
Questions people ask
Why is the tenacity factor 8.826 rather than 9?
Because two conversions are happening at once. Denier is nine times tex, which supplies the 9. But grams per denier measures force in gram-force while centinewtons per tex measures it in centinewtons, and one gram-force is 0.980665 cN. Multiply the two and the factor is 8.825985. Rounding it to 9 makes every converted tenacity about 2% high - small enough to hide inside test scatter, large enough to fail a specification at the margin.
Two yarns have the same tenacity but different MPa. Which one is stronger?
It depends what the yarn has to do. Tenacity is strength per unit mass and is what matters when weight is the constraint - ropes, ballistic panels, aerospace. Megapascals is strength per unit area and is what matters when space is the constraint, or when the yarn is a reinforcement inside a matrix that has a fixed volume to give it. UHMWPE is the clearest case: at 0.97 g/cm3 it dominates on tenacity and loses badly on MPa against an aramid of the same tenacity.
What is breaking length for, if tenacity already says the same thing?
It is the same quantity in units people can picture: the length of yarn that would snap under its own hanging weight. A 45 cN/tex yarn has a breaking length of 45.9 km, so a strand reaching most of the way to the stratosphere would just fail at the top. It survives in rope and cordage work, and in older textile literature, where it predates the tex system entirely.
Does GSM to oz/yd2 depend on the fabric width?
No - both are weights per unit area, so the conversion is a single constant and width never enters it. Width matters only for the linear figures, grams per running metre and ounces per running yard, which is where most of the confusion in fabric buying actually lives: two mills quoting the same GSM at different finished widths are selling rolls of different weight and different cost per metre.