Electronic thread tension meter with a motor-driven take-off for measuring and setting needle and bobbin thread tension on sewing machines, so that thread brakes can be set at a constant take-off speed of 9 m/min. A special fixture also measures the take-off tension of shuttle bobbins. It is based on the ETX tension meter, sits on a vacuum foot next to the sewing machine, and handles threads up to 2000 tex in four measuring ranges.
Yarn testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 2 of 5 key figures recorded
- Yarn test speed (evenness / hairiness)9 m/min
- Force capacity—
- Tensile (crosshead) speed—
- Yarn count range2 000 tex
- Test standards—
- Weight0.84 kg
- Make
Hans SchmidtGermanyhans-schmidt.com (the builder's website, opens in a new tab) All 17 machines from Hans Schmidt - Class
- Yarn testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
- See it
- Exhibited at ITMA ASIA + CITME 2024, Shanghai, stand H8-A04 (as listed by the organiser)
Specification
| Parameter | Value | Unit | Comparable |
|---|---|---|---|
| Measuring range, MST-200 | 1 to 200.0 | cN | |
| Measuring range, MST-500 | 1 to 500.0 | cN | |
| Measuring range, MST-1000 | 1 to 1000 | cN | |
| Measuring range, MST-2000 | 1 to 2000 | cN | |
| Calibration material, MST-200 | PA 0.12 | mm Ø | |
| Calibration material, MST-500 | PA 0.2 | mm Ø | |
| Calibration material, MST-1000 | PA 0.3 | mm Ø | |
| Calibration material, MST-2000 | PA 0.5 | mm Ø | |
| Thread count, max. | 2000 | tex | |
| Accuracy | ±1 % Full Scale ±1 Digit (typically ±0.5 % Full Scale) | ||
| Units | cN, g, N or lb, switchable | ||
| Over-range | ca. 10 | % Full Scale | |
| Overload protection | 200 | % Full Scale | |
| Measuring principle | Strain gauge full bridge | ||
| Measuring roller deflection | 0.5 max. | mm | |
| Signal processing | digital | ||
| Internal measuring frequency | ca. 1 | kHz | |
| Measuring frequency | max. 200 | Hz | |
| Display | Colour TFT 128 x 160 | ||
| Display interval | ca. 2 times per second | ||
| Output signal | USB | ||
| Memory | 60000 readings in 999 series | ||
| Memory modes | 5 | ||
| Vacuum foot measuring height on work surface | 120 to 220 | mm | |
| Motor take-off speed | 9 | m/min | |
| Temperature coefficient, gain | better than ±0.01 & Full Scale /°C | ||
| Temperature range | 10 – 45 | ºC | |
| Humidity | max. 85 | % RH | |
| Power supply | Li-ion battery (approx. 2 h continuous operation), charging time approx. 5 h; mains adapter 100 – 240 V AC | ||
| Housing material | Aluminium | ||
| Weight, instrument (foot) | ca. 840 (500) | g | 0.84 kg |
Read from the builder's published page: www.hans-schmidt.com, on 2026-11-07.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.hans-schmidt.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Hans Schmidt
Other machines of this kind: Yarn testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.