The ZE series are low-cost handheld electronic tension meters for measuring low running tensions of fibres, threads and fine wires. The ZEF has a narrow catch bracket and small guide rollers for confined spaces and is used on circular knitting and textile winding machines; the ZED is used on winding machines for fibres and thin wires. Both measure with a strain gauge full bridge and show readings on a colour TFT display.
Yarn testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 0 of 5 key figures recorded
- Yarn test speed (evenness / hairiness)—
- Force capacity—
- Tensile (crosshead) speed—
- Yarn count range—
- Test standards—
- Weight0.2 kg
- Make
Hans SchmidtGermanyhans-schmidt.com (the builder's website, opens in a new tab) All 17 machines from Hans Schmidt - Class
- Yarn testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
- See it
- Exhibited at ITMA ASIA + CITME 2024, Shanghai, stand H8-A04 (as listed by the organiser)
Specification
| Parameter | Value | Unit | Comparable |
|---|---|---|---|
| Measuring ranges available (series) | von 0.5 - 50 cN bis 1 - 500 cN | ||
| Measuring range, ZEF-50 | 0.5 – 50.0 | cN | |
| Measuring range, ZEF-100 | 0.5 – 100.0 | cN | |
| Measuring range, ZEF-200 | 1.0 – 200.0 | cN | |
| Resolution, ZEF models | 0.1 | cN | |
| Measuring head width, ZEF | 43 | mm | |
| Guide roller groove diameter, ZEF | 7.4 | mm | |
| Material, ZEF | Fibres up to 200 tex or Cu wire Ø 0.16 mm | ||
| Measuring range, ZED-200 | 1.0 – 200.0 | cN | |
| Resolution, ZED-200 | 0.1 | cN | |
| Measuring range, ZED-500 | 1 – 500 | cN | |
| Resolution, ZED-500 | 1 | cN | |
| Measuring head width, ZED | 63 | mm | |
| Calibration material, ZED | PA: 0.20 mm Ø | ||
| Material, ZED | Fibres up to 500 tex or Cu wire Ø 0.28 mm | ||
| Accuracy | ±1 % Full Scale (Messbereichsende) ±1 Digit oder besser typisch ±0.5 % Full Scale | ||
| Units of measure | switchable cN, g, N, lb | ||
| Over-range | ca. 10 | % Full Scale | |
| Overload protection | 200 | % Full Scale | |
| Measuring principle | Strain gauge full bridge | ||
| Measuring roller deflection | max. 0.5 | mm | |
| Internal measuring frequency | ca. 1 | kHz | |
| Measuring frequency | 250 | Hz | |
| Display | Colour TFT 128 x 160 | ||
| Automatic switch-off | after 3 min without use | ||
| Temperature range | 10 – 45 | ºC | |
| Air humidity | max. 85 | % rel. humidity | |
| Power supply | LiPo battery (approx. 25 h continuous operation, charging time approx. 3.5 h), USB plug-in power supply 100 – 240 V AC | ||
| Housing material | Plastic (POM) | ||
| Weight, net (gross) | ca. 200 (600) | g | 0.2 kg |
Read from the builder's published page: www.hans-schmidt.com, on 2026-11-07.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.hans-schmidt.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Hans Schmidt
Other machines of this kind: Yarn testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.