Nantong Hongda HD021E is a yarn testing instrument, still in its builder’s current range. Its builder lists tensile speed 500 mm/min, gauge length 500 mm and maximum elongation 250 mm. Yarn testing instruments measure yarn and fibre properties such as evenness, imperfections, hairiness, tensile strength, elongation, count and twist, as well as fibre length and fineness.
Yarn testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Yarn test speed (evenness / hairiness)—
- Force capacity—
- Tensile (crosshead) speed0.5 m/min
- Yarn count range—
- Test standards—
- Gauge length500 mm
- Max. elongation (stroke)250 mm
- Make
Nantong HongdaChinanthongda.com (the builder's website, opens in a new tab) All 8 machines from Nantong Hongda - Class
- Yarn testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
- See it
- Exhibited at ITMA ASIA + CITME 2024, Shanghai, stand H8-A14 (as listed by the organiser)
Specification
| Parameter | Value | Comparable | As published |
|---|---|---|---|
| Measuring range / accuracy / resolution | 5000cN±0.5% | ||
| Measuring range / accuracy / resolution | 1.0cN | ||
| Measuring range / accuracy / resolution | 12000cN±0.5% | ||
| Gauge length | 500 mm | ||
| Maximum elongation | 250 mm | ||
| Tensile speed | 500 mm/min | 0.5 m/min | |
| Power supply voltage | AC220V | ||
| External dimensions | 600×360×1080 mm | Host |
Read from the builder's published page: www.nthongda.com, on 2026-10-29.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.nthongda.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Nantong Hongda
Other machines of this kind: Yarn testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.