Fabric Inspection Guidelines

Fabric inspection focuses on fault/defect rate color, end to end and edge to middle shading, hand/handle, and appearance. The client will select the appropriate fault rate and standard to determine the acceptance of each shipment. This will minimize the quantity of panels or garments rejected for fabric faults, thereby ensuring the quality of the finished goods.

Fabric Inspection Guidelines Read More »

fabric inspection table

Fabric Inspection and Terms

The quality of a final garment depends on the quality of a fabric when it is received as a roll. Even the most outstanding manufacturing methods cannot compensate for defective materials. Normally, 10% of the rolls received are inspected and evaluated based on a four-point system. This way, fabric related quality problems can be avoided before it is put into production.

Fabric Inspection and Terms Read More »