Coated and laminated textile fabrics

Definitions, applications, and attributes of coated and laminated fabrics

4 23,607

Fabric surface modification is a novel technique by coating and lamination which can improve structural performances. It provides the opportunities to manufacturer the special fabrics like water-proof resistant tarpaulins, coverings, large tents and architectural uses, back coating for upholstery including auto seats, food, medical applications, parachutes, woven curtains, for heat-sensitive fabrics, automotive fabrics, disposable hospital apparel etc. the recent developments also enhanced the lamination and coating technique into state-of-art process of the future in textile field.

Raw-materials and their properties of Coated and Laminated Fabrics

A coated fabric combines the benefits of the base fabric construction plus use of the appropriate polymer with which it is coated. The resulting coated fabric will have many properties which cannot be offered by either component individually, and careful consideration is necessary to select both base fabric and coating polymer. The base fabric provides the mechanical strength of the composite material and supports the layer of coating applied to it. For quality coated fabrics, quality base fabrics are essential.

Base Fabrics

  • Polyester and nylon are the main fibres used, because of their strength and general resistance to moisture, oils, micro-organisms and many common chemicals. Generally, polyester is more resistant to light and ultraviolet (UV) degradation than nylon while nylon is more resistant to hydrolysis. Polyester, however, has grown at the expense of nylon because of its better dimensional stability and shrink resistance, lower extensibility and generally lower cost.
  • High tenacity nylon and polyester yarns are used in many coated articles for extra strength, and aramid fibres are used where more specialist properties, such as high strength to weight ratio and resistance to high temperatures, are required.
  • Acrylic fibres are used for some applications where very high UV resistance is necessary, such as for awnings, car roofs and hoods for convertibles.
  • Cotton was the first fabric used in textile coating and it is still used in large quantities. In applications where strength is required, however, it has been replaced by nylon and polyester.
  • Use of special verities of nylon and polyester, such as high tenacity (HT) and low shrinkage (LS), which are used in coating applications, such as tarpaulins and conveyor belts.
  • Glass woven fabrics are used as bases for PTFE coatings for industrial uses, such as calendar belts and building structures. These applications make specific use of the glass properties of very high strength with very low elongation and excellent flammability resistance.

Adhesives

POLYMER adhesives

Related Posts
1

Manufacturing Process of Automobile Airbags

Manufacturing Airbags from Nylon66 Woven Fabrics

2

Narrow Fabrics – tapes, braids, and webbings

Narrow Fabrics for Industrial, Medical, Automotive, Aerospace, Marine, and Military Uses

3

Carbon Fibre – strong, stiff, & light weight fibres

Properties, process, history, and application of carbon fibres

4

Disposable Baby Diapers

Properties, components, advantages, and uses of modern disposable diapers

Polytetrafluoroethylene, silicone polymethyl, polyethene, polyisoprene, polystyrene, polyvinyl alcohol, polymethyl methacrylate, polyvinyl chloride, polyacrylonitrile, amino cured epoxide, polyethene terephthalate, cellulose, poly hexamethylene adipamide.

Schematic of a coated textile
A demonstrates how a coating covers the surface of the fabric, as applied in liquid form, it is able to penetrate the fabric structure, filling the air pockets and bridging the interstices.
Schematic of a laminated textile
Depicts how a laminate sits on the fabric surface, the fabric retains its air pockets and the laminate has fewer points contacts.

 

As with both lamination and coating, the bonding mechanism is of importance. The bonding can occur through the thermoplastic qualities of the coating or laminate, whereas it is heat set, although this is not appropriate for all materials, so solvent or water-based adhesives are used. The use of adhesives is a highly technical area, as gaining a strong yet flexible bond can be a challenge.

The most important factor with both lamination and coating the bonding mechanism is of prime importance which may occur through the thermoplastic qualities of the coating or laminate, or is heat set, although this is not appropriate for all materials, so solvent or water-based adhesives are used. The use of adhesives is a highly technical area, as gaining a strong yet flexible bond can be a challenge.

Fabric preparation and fabric structure prior to coating is important, particularly for its stabilization, which may impact on the coating or laminate applied

The end product is sometimes referred to as a composite, as it is a composition of a textile and non-textile component. Many of the mechanical properties are determined by the fabric, such as tear strength, the coating largely determines the chemical properties, and the handle is often determined by both.

It is not just technical applications which utilize coating and lamination technology, the fast-paced fashion market is constantly giving the technology new challenges with the need to create innovative and visually interesting looks such as a high shine, futuristic finish, or imitation animal skin.

Pages ( 3 of 4 ): « Previous12 3 4Next »
4 Comments
  1. brandanimators says

    Thanks for sharing.
    Brand Animators – Bringing Your Vision to Life with Innovative Video Solutions. From start-ups to large corporations, every business has a unique story to tell. At Brand Animators, our mission is to help you tell that story in a captivating and memorable way. As a top quality 3d, 2d animation video production company in Houston, Texas and best explainer video company in San Antonio, Texas and professional Healthcare & Medical animation video making studio in Dallas, Texas offer services such as 2d animation videos 3d animation videos, Motion graphics, 3d medical animation, Healthcare videos, Corporate films, Whiteboard animation videos, 3d Architectural walkthrough animation, Marketing and training videos, Product videos. And more! Whether you’re looking to promote your brand, educate your audience, or simply convey information in an engaging and visually appealing manner, Brand Animators has you covered. Our video solutions are tailored to your budget, timeline, and company objectives.

  2. Alice Carroll says

    Thanks for the pointing out that combine fabric is also a term that means the same things as coated fabrics. I will keep that in mind when shopping for PVC-coated fabrics in the future. I might miss some products when browsing from using the wrong terminology.

    https://www.rhinotex.com/pvc-fabric-products

  3. ashok hakoo says

    You can contact me for any advise on technical fabrics.

  4. Sunil Kasat says

    In search of Proper consultant for technical textile & coating industry

Leave A Reply

Your email address will not be published.