Home » Fiber & Yarns » Yarn » Optimum Yarn Spinning conditions

Optimum Yarn Spinning conditions

Factors governing Optimum Spinning condition, Yarn quality assessment, Causes of end breakage/ end down

yarn spinning

Factors governing optimum spinning conditions

  • Spindle speed
  • Ring die
  • Lift
  • Traveler weight
  • Relative humidity

Yarn quality assessment

  • Yarn count and its variation
  • Twist and its variation
  • Evenness CV% or U%
  • Strength and its variation(csp of yarn)
  • Imperfections

Causes of end breakage/End down:

If spinning tension is greater than yarn strength in the Ring frame, then end breakage is occurred and also due to roller lapping.

A. Technical causes

  • An insufficient twist in the yarn
  • If traveler fly off
  • Subbing thorough
  • Stretched roving
  • Faulty drafting roller setting
  • Faulty traveler selection
  • Excessive yarn tension
  • Improper atmospheric condition

B. Mechanical Causes

  • Faulty drafting system
  • Worn out ring and traveler
  • Faulty gear and wheels
  • Worn out top rollers
  • Faulty apron
  • Spindle vibration
  • Eccentric ring

Optimum spinning conditions

  1. Spindle speed
  2. Ring die
  3. Lift
  4. Traveler weight
  5. Relative humidity

Yarn quality assessment

  • Yarn count and its variation
  • Twist and its variation
  • Evenness CV% or U%
  • Strength and its variation(csp of yarn)
  • Imperfections

Causes of end breakage/End down:

If spinning tension is greater than yarn strength in the Ring frame, then end breakage is occurred and also due to roller lapping.

A. The technical causes

  • The insufficient twist in the yarn
  • If traveler fly off
  • Subbing thorough
  • Stretched roving
  • Faulty drafting roller setting
  • Faulty traveler selection
  • Excessive yarn tension
  • Improper atmospheric condition

B. Mechanical Causes

  • Faulty drafting system
  • Worn out ring and traveler
  • Faulty gear and wheels
  • Worn out top rollers
  • Faulty apron
  • Spindle vibration
  • Eccentric ring

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device

The Selvedge · free · one email a week

Know what changed in textiles this week.

Our register tracks 3,130 textile standards. Nobody reads them all, so once a week we tell you which ones moved, and what else is new.

  • Standards added, revised or withdrawn that week
  • One textile calculation, worked through to its answer
  • New and revised guides on the site
  • Textile fairs coming up, with their dates

Free when you confirm: Spinning and Weaving Calculations (PDF). 49 calculations, from the blowroom to the loom, each with its formulas and a worked example.

We send a confirmation link first. Unsubscribe in one click, any time.

  • No spam
  • Your address is not shared
  • Unsubscribe in one click