ISO 1833-26
Textiles — Quantitative chemical analysis — Part 26: Mixtures of melamine with certain other fibres (method using hot formic acid)
Melamine fibres separated using hot formic acid. Melamine is a flame-resistant fibre found in protective clothing and upholstery, and blends containing it are usually being tested because a…