Study on application of reduced Graphene Oxide on cotton fabric for Breathable Waterproof finish

This article explains the application of reduced graphene oxide on cotton woven fabric to achieve breathable waterproof finishing. After finishing the fabric was analysed various morphological properties as well as physical properties to confirm comfortability.