Skip and Pointed Twills

Skip twills are a type of broken twill effects formed by a skip drawing-in draft and a regular twill weave as a chain draft. The weaves that form a wave effects across the cloth known as pointed twills. These effects are also frequently…
Read More...

Fancy Twills

The fancy twill is formed by placing small spots between the main lines of twill. The first end of the weave should be a continuation of the last end and the first pick should be a continuation of the last pick, so that the weave will…
Read More...

Twill Weave Derivatives

Certain weaves, based on their construction or use our group into categories, For instance, the plain weave may be considered as a standard construction.One of the largest of these classes is that of twill weaves, which are so called…
Read More...