Traditional weaving is cloth made on hand-worked looms whose build, techniques and patterns a community has passed down: a lengthwise warp is held taut, and a crosswise weft is passed through an opening in it, the shed, and beaten into place. Methods around the world differ in three ways. They differ in how the warp is held taut: by the weaver’s body (backstrap loom), by stakes in the ground (ground loom), by hanging weights (warp-weighted loom) or by a fixed frame. They differ in how the shed is opened: by a shed rod and string heddles lifted by hand, by turning tablets, or by treadles worked with the feet. And they differ in how the pattern gets in: by dyeing the yarn before weaving (ikat), by inlaying extra weft only where a motif sits (jamdani, songket) or by weaving each colour area on its own (kilim, Navajo tapestry). The table below compares thirteen methods, from the backstrap loom to the pit looms of South Asia, the narrow-strip looms of kente and the two-person drawloom of Nanjing brocade, with the heritage listing each holds.
Last verified: 11 October 2026. Each method is described from a museum record, a UNESCO inscription, a government register or a first-hand account, linked where it is used. Sources are listed at the end.
Traditional weaving methods at a glance
| Method | Loom, and how the warp is held | How the shed is opened | The cloth | Where | Heritage listing |
|---|---|---|---|---|---|
| Backstrap (loin) loom | Between a bar fixed to a wall or post and a bar at the weaver’s waist; a strap round her back takes the strain | Heddle bar lifted by one hand, a bamboo bar pressed down by the other; a flat sword holds the shed and beats | Garment cloths, belts, dance dresses; nearly any weave | Northeast India; Japan; Guatemala (Maya) | Yūki-tsumugi silk, woven on a back-tension loom: UNESCO, 2010 |
| Staked ground loom | Two beams pegged to the ground, the warp flat between them | Rods lifted by hand, as on the backstrap loom | Warp-faced plain weave (Al Sadu); belts and garments (Taquile); pile carpets (Fars) | Arabian Peninsula; Lake Titicaca, Peru; south-west Iran | Al Sadu: UNESCO, 2020, Qatar added 2025; Taquile, 2008; Fars, 2010 |
| Warp-weighted loom | Upright; the warp hangs from a top beam, tied in bundles to loom weights | A heddle bar pulled against a fixed shed rod; the cloth grows downward from the top beam | Wool cloth | Ancient Greece and Europe; the Sámi of Norway and Finland into the 1950s | None |
| Navajo upright loom | A continuous warp between two beams on a two-post frame; the cloth is folded down and sewn to the fixed lower beam | Shed rod for one shed, string healds on a rod for the other, widened with a flat batten; four sheds for twills | Weft-faced wool blankets and rugs, alike on both faces | Navajo (Diné) Nation, US Southwest | None: the US is not party to UNESCO’s 2003 Convention |
| Tapestry rug (kilim) | Upright or horizontal loom | Plain-weave sheds; each colour’s weft turns back at its own edge, leaving slits where colours meet | Flat-woven rugs, the weft hiding the warp: 6 warp ends and about 26 picks per inch in one Turkish example | Turkey, the Caucasus, Central Asia | Wall carpets of Romania and Moldova, vertical or horizontal looms: UNESCO, 2016 |
| Knotted pile carpet | The dar loom (Kashan); a horizontal frame on the ground (Fars) | Plain-weave ground with rows of knots tied onto the warp | Pile carpets; asymmetrical (Farsi) knot on cotton or silk in Kashan | Iran | Kashan, 2010; Fars, 2010 |
| Pit loom | A frame on four posts fixed in the ground over a pit; warp beam behind, cloth beam in front | Treadles in the pit work the heddles; the hands throw the shuttle (or pull a fly-shuttle cord) and swing the sley to beat | Plain and patterned cloth; the fly-shuttle version weaves superfine yarn but not intricate extra-weft patterns | India, where the fly-shuttle pit loom is the commonest handloom outside Assam | India’s Handlooms Act, 1985, can reserve articles for handlooms alone |
| Narrow-strip loom (kente) | A small horizontal loom with two or three sets of heddles | One pair of heddles weaves the plain ground; another set, threaded in groups, lifts the warp for the weft-faced pattern blocks | Strips about 10 cm wide, warp-striped, sewn edge to edge | Ghana (Asante and Ewe) | Kente: UNESCO, 2024 |
| Floor treadle loom | A fixed frame with warp and cloth beams | Treadles (two on the Malay kek) lift the shafts | Songket, with gold or silver thread; Harris Tweed, wool woven at home | Malaysia; Outer Hebrides, Scotland | Songket, UNESCO, 2021; Harris Tweed Act 1993 |
| Drawloom | A large loom worked by two people, one above, one weaving below | Pattern threads lifted from above while the weaver works the ground weave | Silk brocade with gold and peacock-feather yarn | Nanjing, China | UNESCO, 2009 |
| Tablet (card) weaving | No frame: the warp is stretched between two fixed points | Each end passes through a hole in a tablet; turning the pack brings new threads to the top | Narrow bands of twisted warp cords | Viking-age Norway: 48 bands in the Oseberg burial of 834 | None |
| Ikat | Any loom | Ordinary sheds; the pattern is tied and dyed into the yarn before weaving | Soft-edged motifs; in double ikat warp and weft must line up | India (Gujarat, Telangana); Japan; Indonesia | GI: Pochampally Ikat (2004), Patan Patola (2013) |
| Jamdani | Handloom | Ground sheds as usual; motifs made with discontinuous wefts that run only across each motif | Sheer cotton with woven-in motifs | Around Dhaka; Uppada, Andhra Pradesh | UNESCO, 2013; Uppada Jamdani Sarees GI (2009) |
Years are the year of inscription on a UNESCO list or of a geographical indication (GI) certificate in India’s register. A listing recognises a named practice in a named place. It is not a ranking, and many old methods have none.
What is traditional weaving?
Weaving interlaces two sets of threads at right angles: the warp, set up first and held under tension, and the weft, passed across it one pick at a time. Every loom repeats three motions, which the Indira Gandhi National Centre for the Arts names in its account of Indian looms: shedding (separating the warp into two layers), picking (passing the weft) and beating (pressing the pick against the cloth) (IGNCA). Traditional weaving does this on looms worked by hand or foot, to designs and rules handed down. Indian law draws the line at the motor: the Handlooms (Reservation of Articles for Production) Act, 1985 defines a handloom as “any loom, other than power loom” and lets the government reserve articles for handlooms alone (the site’s record of the Act).
A method is not the same as a weave: plain, twill and satin are structures any of these looms can make (see the classification of weave patterns). The industrial looms that followed are in the history and evolution of looms.
How a loom makes the shed
Every loom lifts part of the warp so the weft can pass under it. The oldest way needs only sticks and string, and it works the same on backstrap, ground and upright looms. Washington Matthews watched Navajo weavers do it and set it down in 1884 (Navajo Weavers, Bureau of Ethnology):
- Lay the warp as one continuous string in a figure of eight between two poles. The crossing makes the two sheds at the start, and they stay apart for the whole work.
- Hold one shed with a rod. The shed rod, which carries no heddles, keeps that shed open.
- Tie heddles to the other layer: a string loop round each of its threads, the loops carried on a heddle (heald) rod.
- Pull the heddle rod forward. Its threads come through and open the second shed about an inch.
- Widen it. A flat oak batten goes in edgewise and is turned flat, propping the shed about 3 inches open. The weft is passed.
- Beat. A wooden fork, the reed-fork, presses the weft down; the batten, edgewise again, strikes it home.
- Change sheds. Release the heddles and push the shed rod down to reopen the first shed. Repeat.

A plain weave needs only those two sheds; a twill needs more. For diagonal weaves Matthews saw the warp divided into four sheds, one on a shed rod and three on heald rods, opened in the order 1, 2, 3, 4; the reverse order turned the diagonal, and with the healds arranged differently on the warp the same mechanism wove diamonds. The site’s weave calculator gives the same count from the notation: a plain weave repeats on 2 ends and needs 2 shafts, a 2/2 twill on 4 ends with 4 shafts. Treadle looms make the same lifts with shafts tied to pedals (weaving loom types); tablet weaving turns cards; the drawloom adds cords, pulled from above, that lift only the pattern threads.
Traditional looms around the world
Backstrap loom
On a backstrap loom the weaver’s body is part of the loom. On the loin, or back strap, loom that IGNCA describes in Manipur, Tripura and parts of Assam, a front bar hangs between two loops fixed to the house wall and the warp runs to a breast bar at the weaver’s waist. A strap of leather or cloth passes round her back, and she braces her legs against an adjustable footrest to set the tension. She lifts the heddle bar with her left hand while pressing a bamboo bar down with her right, holds the shed with a flat wooden sword, passes a bamboo shuttle and beats with the sword. With no fixed frame, the loom is cheap and portable (IGNCA). Maya women in Guatemala weave on backstrap looms today, and ancient ceramic figurines show women weaving on them the same way (ReVista, Harvard University). In Japan, Yūki-tsumugi pongee is woven on a back-tension loom from hand-spun silk floss, patterned by tying bundles of yarn before dyeing (UNESCO, 2010).
Ground looms
Pegging both beams to the ground frees the weaver from holding the tension. A predynastic bowl from Badari in Egypt, of the fourth millennium BC, carries a design of long parallel threads crossed by short lines that is read as a loom seen from above (Petrie Museum UC 9547; PONDA). Three living traditions on UNESCO’s lists use ground looms. Al Sadu, Arabic for weaving done in a horizontal style, is a tight, durable, warp-faced plain weave made by Bedouin women from local natural fibres (UNESCO, 2020). On Taquile, an island in Lake Titicaca, cloth is woven on pre-Hispanic ground looms staked with four stakes, and the calendar waistband, a wide woven belt, depicts the year’s ritual and farming cycle (UNESCO, 2008). In Fars, in south-west Iran, women design, colour and weave carpets on a horizontal frame placed on the ground (UNESCO, 2010).
Warp-weighted loom
This upright loom has a cloth beam at the top resting on two side poles. The warp hangs from it, kept taut by loom weights tied to bundles of threads, and the woven cloth is pushed up toward the top beam (Textile Research Centre, Leiden). An Athenian oil flask of about 550 to 530 BC, attributed to the Amasis Painter, shows two women weaving standing at one, the warp tied to weights, beside women weighing and spinning wool (Metropolitan Museum of Art, 31.11.10). In the 1950s Marta Hoffmann found women among the Sámi of Norway and Finland still weaving on it, chiefly heavy woollen bedspreads, and published the study as The Warp-Weighted Loom (1964; summarised by the Textile Research Centre, Leiden). Its place in early cloth-making is covered in early textile production: hand spinning and weaving.
Navajo upright loom
Matthews describes two posts set in the ground and lashed with cross-pieces, or two convenient trees. The warp is bound to an upper and a lower beam, and the lower beam does not turn: the weaver sits on the ground and weaves upward, and when the work rises out of reach she lowers the upper beam, folds the cloth and sews the fold to the lower beam. The batten is rarely over 3 feet long, so the weft crosses only that much warp at a time. Each colour area has its own weft; across one row of a very fine blanket he counted 29. The blankets are single-ply, with the design alike on both faces. Matthews thought it likely, though “by no means certain”, that the Navajo learned weaving from the Pueblo peoples after the Spanish came, and he noted that while most weavers were women, a few men wove, and among them were the tribe’s best weavers (Matthews, 1884).
Pit looms and floor treadle looms
Treadles move the shedding to the feet. IGNCA’s throw-shuttle loom is a frame fitted to four posts fixed in the ground; healds worked by foot make the shed, the shuttle is thrown by hand, and a bamboo reed in a swinging sley beats the weft. Set over a pit in the floor, with the treadles in the pit, it is the throw-shuttle pit loom. The fly-shuttle pit loom adds two shuttle boxes and a string-driven picker that throws the shuttle from box to box. IGNCA calls it the most popular handloom in India except in Assam, says it raised output three to four times, and notes what it gives up: intricate extra-weft patterns (IGNCA).

Two listed traditions use floor looms with treadles. Malaysian songket is woven on a two-pedal floor loom, the kek, by inserting gold or silver thread between the base threads; women weave, and men help make the equipment (UNESCO, 2021). Harris Tweed is defined by an Act of Parliament as cloth “handwoven by the islanders at their homes in the Outer Hebrides, finished in the Outer Hebrides, and made from pure virgin wool dyed and spun in the Outer Hebrides” (Harris Tweed Act 1993, quoted by the Harris Tweed Authority), and all of it is woven on a treadle loom at an islander’s home, not in a mill (Harris Tweed Authority).
Narrow-strip looms: kente
Kente is cloth made of narrow strips sewn together. The Victoria and Albert Museum says Asante and Ewe men traditionally wove the strips on a small double-heddle handloom, typically warp-striped and often with weft-float patterns, and set them so the patterns alternate and offset. UNESCO describes double and triple heddle looms. On these, one pair of heddles weaves the plain ground and the extra set, threaded in groups, lifts the warp for the pattern blocks. One Ewe cloth in its collection is 19 strips, each about 10 cm wide and 280 cm long (V&A). The museum dates kente to at least the 17th century and notes it was historically reserved for royalty and the elite (V&A). UNESCO’s 2024 inscription describes strips of silk, cotton or rayon woven on horizontal looms, with women and men both involved: women chiefly weaving and spinning cotton, men making the looms and tools (UNESCO).
Drawlooms: Nanjing brocade
A figured silk needs its pattern threads lifted separately, pick after pick, and the drawloom does it with cords worked from above. For Nanjing yunjin brocade, two craftspeople operate the upper and lower parts of a large, complicated loom, weaving silk with gold and peacock-feather yarn and singing mnemonic ballads that recall the steps (UNESCO, 2009). The Jacquard mechanism later replaced the cord-puller with punched cards; see Jacquard weaving.
Tablet weaving
Tablet weaving needs no frame. Each warp thread runs through a hole in a flat tablet, commonly four holes to a tablet, and the tablets stand on edge side by side. A quarter turn of the pack brings a new set of threads to the top and opens the next shed; as each tablet’s threads twist round one another, the band is built of twisted cords. The textiles from the Oseberg ship burial in Norway, dated 834, are among the most important finds of the Viking Age and include 48 tablet-woven bands (Skogsaas, EXARC Journal, 2022).
Traditional weaving techniques: how the pattern gets in
Ikat: the pattern is dyed into the yarn
Ikat, a Malay term, is a tie-resist technique: the yarn is tied in bundles and dyed before weaving, so the tied parts resist the dye and the pattern is in the threads before they reach the loom. The soft, blurred edges of the pattern come from the threads shifting slightly as they are woven (V&A). Tying the warp gives warp ikat, as in an 18th-century shawl from Sumba in Indonesia (V&A); tying the weft gives weft ikat; tying both gives double ikat. For a Gujarati patolu made for the Indonesian market, the V&A explains, weavers tied and dyed both warp and weft in patterns, then wove them together so the design formed on both sides (V&A). Pochampally Ikat of Telangana, application 4 on India’s GI register, was certified on 31 December 2004 (GI Registry), and Patan Patola, the double ikat of Gujarat, on 9 September 2013 (GI Registry).
Extra weft: jamdani, songket and brocade
A supplementary weft is an extra pattern thread laid in alongside the ground weave. Jamdani, a sheer cotton from around Dhaka, is slow and labour-intensive because its rich motifs are made directly on the loom with discontinuous wefts, each running only across its own motif (UNESCO, 2013). Uppada Jamdani Sarees of Andhra Pradesh were certified as a GI on 5 March 2009 (GI Registry). Songket lays gold or silver thread between the base threads, and kente strips carry weft floats over a warp-striped ground. Banaras Brocades and Sarees, from Varanasi, were certified as a GI on 4 September 2009 (GI Registry).
Tapestry, warp-faced and knotted pile
In tapestry each colour’s weft is woven back and forth across its own area and packed so densely that it hides the warp. Where two colours meet along a warp thread and both turn back, a slit opens: the slit tapestry of the kilim. A 19th-century Turkish slit-tapestry carpet in the V&A has a wool warp of 6 threads per inch and a weft averaging about 26 per inch, with interrupted vertical slits (V&A). Navajo blankets are weft-faced the same way; pictorial tapestry is covered in tapestry weaving. Warp-faced weaving is the reverse: the warp is set so close it hides the weft, and the design is in the warp colours, as in Al Sadu and the stripes of kente. A knotted carpet adds a pile; in Kashan, wool or silk yarns are knotted to a cotton or silk warp with the asymmetrical Farsi knot (UNESCO, 2010).
Read the cloth: clues to the method
A finished textile usually shows how it was made. Use this on a cloth in a museum, a market or a class collection.
| What you see | What it points to | Checked against |
|---|---|---|
| Narrow strips, about 10 cm wide, sewn edge to edge | A narrow-strip loom, as for kente | V&A kente: 19 strips about 10 by 280 cm |
| The weft hides the warp; short vertical slits where colours meet | Slit tapestry (kilim) | V&A Turkish carpet: 6 warp ends, about 26 picks per inch |
| The warp hides the weft; stripes run lengthwise | Warp-faced weaving, as in Al Sadu | UNESCO, Al Sadu |
| No cut warp ends: cords along both ends and both sides | A continuous warp between two beams, as on the Navajo loom | Matthews: three-ply cords at the ends, twisted cords at the sides |
| The same design on both faces, many separate wefts in one row | Tapestry weaving | Matthews: 29 wefts across one row |
| Motifs with soft, blurred edges, the colour in the yarn, not on the surface | Ikat; double ikat if the pattern is in both warp and weft | V&A ikat gown and patola |
| Extra pattern threads that stop at the edge of each motif | Discontinuous supplementary weft (jamdani) | UNESCO, jamdani |
| Gold or silver thread only in the pattern areas | Supplementary weft, as in songket | UNESCO, songket |
| Tufts of yarn knotted onto the warp, forming a pile | A knotted carpet | UNESCO, Kashan |
| A narrow band whose warp is twisted into cords | Tablet weaving | EXARC, the Oseberg bands |
What is used in weaving traditional cloth
A loom is a set of simple tools, each with one job. The names change from place to place; the jobs do not.
| Tool | Its job | Traditional forms |
|---|---|---|
| Beams, bars or posts | Hold the ends of the warp apart | Bars of the backstrap loom; four stakes of a ground loom; posts and beams of the Navajo loom; four posts of a pit loom |
| Tensioner | Keeps the warp taut | Back strap and footrest; loom weights; a fixed frame |
| Shed rod or lease rod | Holds one shed open, or keeps the threads in order | The Navajo shed-rod; the lease rod of the loin loom |
| Heddles (healds) | Lift the other layer of warp | String loops on a rod; heddle frames on treadle looms |
| Treadles | Work the heddles by foot | The pit loom; the two-pedal kek |
| Sword or batten | Widens the shed and beats the weft | The wooden sword of the loin loom; the Navajo oak batten |
| Comb, reed-fork or reed | Spaces the warp and presses the weft home | The Navajo reed-fork; the bamboo reed of the pit loom |
| Shuttle | Carries the weft | A bamboo shuttle; a twig or a small ball pushed through by hand; the fly shuttle |
| Tablets | Open the shed by turning | Flat tablets, often with four holes |
The fibres are those of the place: wool for Navajo blankets, kilims and Harris Tweed; cotton for jamdani and the tais of Timor-Leste; hand-spun silk floss for Yūki-tsumugi; silk, cotton or rayon for kente; gold or silver thread for songket.

Style, function and convention in textile weaving
- Style: what it looks like. Fibre, colour, motif and structure together. The V&A notes that Asante kente favours geometric patterns in silk, while Ewe weavers add figurative motifs such as animals, people and letters (V&A). In Timor-Leste the colours and motifs of tais vary from one group to the next (UNESCO).
- Function: what it is for. Clothing first, then much else. The wall carpets of Romania and Moldova were decoration and insulation, part of a bride’s dowry and, at funerals, a symbol of the soul’s passage to the hereafter (UNESCO). Tais welcomes newborns, is worn at ceremonies and is given in dowries.
- Convention: the rules around it. Who weaves: making tais is reserved for women, while men gather dye plants and make the equipment. What a design is called: kente is named with proverbs, sayings and social situations (UNESCO). Who may wear it: in Indonesia, patola were for the elite, and court sumptuary laws at times forbade them to commoners (V&A). What may carry the name: Harris Tweed by statute, Pochampally Ikat or Patan Patola by geographical indication.

Where weaving began
Woven cloth is far older than any surviving loom. Impressions of plain-woven and twined cloth on small clay fragments from the Czech Republic date from the Gravettian, roughly 25,000 years ago (Soffer, Adovasio and Hyland, Current Anthropology, 2000; University of Illinois release). One of the oldest pictures of a loom is the horizontal loom read on the Badari bowl; an Athenian flask of the sixth century BC shows the warp-weighted loom in detail. The longer story is in early textile production and the history of looms.
Questions
What is traditional weaving?
Making cloth on hand- or foot-worked looms whose build, techniques and patterns a community has passed down, such as backstrap, ground, upright, pit and narrow-strip looms. The weaver holds the warp taut, opens a shed, passes the weft and beats it in, over and over.
What is used in weaving traditional cloth?
A loom: bars, stakes, posts or weights to hold the warp taut; a shed rod and heddles to part it; a sword or batten to open the shed and beat; and a shuttle or stick to carry the weft. Treadle looms add pedals. The yarn is local fibre such as wool, cotton, silk or hemp.
What are the style, function and conventions of textile weaving?
Style is how the cloth looks: fibres, colours, motifs and structure. Function is what it is for, from clothing to dowry, ceremony and status. Conventions are the community’s rules: who weaves, which patterns are used and what they are called, who may wear the cloth and what may carry its name.
Which weaving tradition ties the warp threads before dyeing?
Ikat. The yarn is tied in bundles and dyed so the pattern is in the threads before weaving. Warp ikat ties only the warp; double ikat, such as Patan patola, ties warp and weft, which must then line up as the cloth is woven.
What rug weaving traditions exist around the world?
Flat-woven tapestry rugs such as the kilims of Turkey, the Caucasus and Central Asia; Navajo rugs woven on an upright loom; the knotted pile carpets of Kashan and Fars in Iran; and the wall carpets of Romania and Moldova. The Iranian, Romanian and Moldovan traditions are on UNESCO’s Representative List.
Where did weaving originate?
No single place is known. Among the oldest evidence are impressions of woven cloth on clay fragments from the Czech Republic, about 25,000 years old. One of the oldest pictures of a loom, read as a horizontal loom seen from above, is on a predynastic Egyptian bowl from Badari of the fourth millennium BC.
Sources
- W. Matthews, “Navajo Weavers”, Third Annual Report of the Bureau of Ethnology, 1881–82 (1884), pp. 371–392, Project Gutenberg.
- Indira Gandhi National Centre for the Arts, Types of Looms; the Handlooms (Reservation of Articles for Production) Act, 1985 (Act No. 22 of 1985), sections 2 and 3, text.
- UNESCO intangible cultural heritage: Yūki-tsumugi; Al Sadu and its extension; Taquile; Fars; Kashan; wall carpets; kente; songket; yunjin brocade; jamdani; tais.
- Victoria and Albert Museum, kente O164606 and O263818, ikat O114688 and O455656, patola O17103, slit-tapestry carpet O122058; Metropolitan Museum of Art, 31.11.10; Petrie Museum UC 9547 via PONDA.
- Intellectual Property India, GI Registry, applications 4, 99, 122 and 232.
- Textile Research Centre, Leiden, What is a warp-weighted loom?; M. Hoffmann, The Warp-Weighted Loom (Universitetsforlaget, 1964).
- B. Skogsaas, “A Tablet Woven Band from the Oseberg Grave”, EXARC Journal (2022); H. Nottebohm, “Maya Weaving Heritage”, ReVista (2010); O. Soffer, J. M. Adovasio and D. C. Hyland, Current Anthropology 41 (2000).
- Harris Tweed Authority, Our role (the 1993 Act’s definition) and Weaving.
How this page is kept
Last verified: 11 October 2026. Loom mechanics come from first-hand and institutional accounts (Matthews; IGNCA), heritage listings from the UNESCO decision or element page and the Indian GI Registry entry, and thread counts and strip sizes from the museum’s own catalogue record, each read on that date. Where a museum and UNESCO describe a tradition differently, as for who weaves kente, both are given. Facts that could not be traced to such a source were left out. The weave calculator links use the site’s tool as it stood on this date.
Change log. 11 October 2026: rewritten in full around a sourced comparison of thirteen methods. Removed: unsourced case studies (a West Bengal cooperative’s “25%” efficiency gain, an unnamed Italian luxury brand, a semi-automated kente mill); sections on markets, stakeholders and digital looms that described no traditional method; and Jacquard weaving listed as a traditional regional method. Corrected: the Navajo are one nation, not several “tribes”; the pit loom is not a loom “ideal for narrow, delicate fabrics” but, in its fly-shuttle form, the commonest handloom in India. Added: the heritage listing of each method. Dropped images that did not show traditional weaving: a modern sample loom, a computer rendering of an exhibition, a world-map puzzle and a fibre-craft class.
Found an error? Please tell us through the contact page, naming the section and the source that disagrees.