textile articles repository

Cotton Fibers – the king of fibers

Cellulose-seed fiber from the nature

18 61,211

Cotton fiber is a soft staple fiber that is grown in a form known as a boll around the seeds of the cotton plant, a shrub native to tropical and subtropical regions.

Classing Cotton

Cotton buyers judge cotton on the basis of samples cut from the bales. Skilled cotton classers grade or “class” the cotton according to standards established by the US Department of Agriculture such as cleanliness, the degree of whiteness, length of the fiber, and fiber strength.

The classers pull a sample; they discard most of the cotton until just a pinch of well-aligned fibers remains. They measure the length of the fibers, referred to as staple fibers. Longer staple fibers are higher-grade cotton and are sold at higher prices. Long staples range from 1.1 inches to 1.4 inches long.

The USTER® HVI classing is the standard classification system in the United States and also for the international cotton trade. USTER® HVI is used for measurement of the most important cotton fiber properties of micronaire, fiber length (UHML), uniformity, short fiber index, strength, elongation, color, trash content, and degree of maturity. HVI classing has been available to all growers since 1981.

Types of Cotton fabric

Quilting Cotton

Quilting cotton is also referred to as craft cotton, patchwork cotton, or printed cotton and is plain weave cotton that is light to medium weight cotton. They are a pretty closely woven fabric and there are an array of quilted cotton fabrics available that are utilized for making tops, tunics, aprons, blankets, quilts, dresses, and skirts.

Brushed Cotton

Brushed cotton is sometimes referred to as flannel or flannelette. it is a medium-weight cotton fabric that has surface fibers that are brushed on one side of the material which gives it hey very soft and warm look and feels. you can purchase it in plain material, or checked printed or stripe material and it is most often used for casual shirts, children’s clothing, and linings for bedding comic coats, and jackets. When it comes to a lightweight flannelette, it is used many times to make nightgowns and pajamas.

Pima Cotton

Considered a higher-end type of cotton fabric, Pima cotton boasts longer fibers than regular cotton. Smooth fabric that is very soft to the touch is created with Pima cotton. It tends to be resistant to wrinkles and very durable. Several products are created from this type of fabric, including bed sheets and underwear.

Egyptian Cotton

Known as the highest quality cotton fabric, Egyptian cotton is used to make a number of products, including higher thread count bed sheets that many people prefer over other types of sheets to sleep upon. You can expect to pay a little more at the cash register for anything made from this type of fabric.

Cotton Twill

There are many fabrics that are created from a cotton twill weave fabric, including some linen fabrics, denim, chino, and gabardine. It is used in making pants, jackets, skirts, and much more. It is distinguished by its weave pattern that places diagonal lines in the fabric and it is very sturdy and durable. Cotton twill is also used in creating some types of upholstery fabric since it is so durable.

Cotton Lawn

Cotton lawn is a lightweight, plain-weave cotton fabric that has a crisp, smooth feel. It can be quite sheer but is reasonably strong due to the fine weave. Often used for blouses, children’s clothes, tablecloths, and blankets.

Organic Cotton

Related Posts
1

Cotton Fibers and its Properties

Properties, classification, and methods to identify the attributes of cotton fibers

Organic cotton fabric is created without any synthetic fiber being added into it and is usually free of chemicals, including fertilizers and pesticides, when the cotton is being grown by cotton producers.

Levant Cotton

Levant cotton comes from the Levant seeds of the Gossypium herbaceum cotton plant, which are also used for feed, oil extraction, and food. It is considered Old World cotton and is used by many commercial cotton producers in creating clothing and other products.

Wool Fabric

With cotton wool fabric you end up with the best of both types of fibers: cotton fiber and wool fiber. This means you get the comfort of cotton with the resilience and strength from the wool fiber. This type of cotton blend can be worn all year round no matter what season it is outside. Cotton and wool blends are normally used in higher-end clothing, including tweed, chenille, brocade, and velvet.

Poplin

Poplin, also known as cotton broadcloth, is a medium-weight, plain-weave cotton fabric that is tightly woven and easy to work with when sewing. It is extremely versatile and is used often to produce blouses, dresses, and shirts. It can be a pure cotton blend or one that includes polyester fabric.

Linen Cotton

The linen-cotton mix fabric is very soft and light to medium-weight. It often contains a blend of 50 percent linen and 50 percent cotton. It retains the look and feel of linen but is more robust and will not crease as much. Some clothing made from linen and cotton is a little itchy to your skin. Some products created with linen cotton fabric include skirts, sheets, jackets, and dresses.

Cotton Silk

A mix of silk and cotton weave produces a lightweight fabric that is very soft to the touch and offers the drape and luster that silk provides. It is used most often to make blouses and dresses.

Sea Island Cotton

Sea Island cotton is the rarest type of cotton fabric type in the world as well as one of the finest versions of cotton fabric. It boasts a very fine, uniform texture that offers a silky luster and feels great next to your skin. A variety of products are made from Sea Island cotton, including high-end men’s boxer shorts.

Voile

Voile is a soft and very sheer fabric type that is typically made of 100 percent cotton or of cotton blended with linen or polyester. It is a very lightweight cotton fabric that gets its name from the French term for veil. This fabric is used often in hot, tropical climates and for mosquito netting and sheer curtains for windows.

Poly Cotton

Polycotton is usually a blend of 50 percent polyester and 50 percent cotton can sometimes be made of 65 percent cotton and polyester. It is a very lightweight plain-weave fabric that is very strong, durable, resistant to creasing, however, it is less breathable than other cotton fabrics so it can be hot and make you sweat if you wear it during the warmer months. It is often used to create children’s clothing, skirts, and aprons.

Cotton Drill

This durable fabric is known for being a very dense, strong, medium to the heavyweight fabric which is a popular choice for uniforms and work clothes. It’s very similar to the texture and diagonal weave of denim, but is usually dyed and has a smoother appearance, making it perfect for all sorts of garments – including tailored and casual designs. It is easy and comfortable to wear, and its use has become progressively more stylish and contemporary.

Pages ( 4 of 5 ): « Previous123 4 5Next »
18 Comments
  1. Abubakar says

    Thank you so much. This article is very good and i learned a lot. I think I will share it with all my friends on instagram so that they can enjoy reading a good article like this. Also, check out this article on MKBHD Smartphone Awards, it is pretty good too.

  2. Jim says

    Sorry, I saw a typo in my email address in prior comment.
    It is corrected here.

  3. Dotun Ajibola says

    wow this article is well informative and constructive. thank you
    It was worth the reading.

  4. gami says

    great content ….well written, i was able to learn something new on cotton fibers you can also check out this Whatsapp plus 2022 and this Life of Mellow mod APK

  5. Mia Stark says

    This is truly an amazing write-up you have here. I must confess that I was impressed by the first few paragraphs. This goes without saying you make an amazing blogger and your information is right on point. If you are ever interested in guest posting, you can check out my site at death run and football stars

    https://www.cinegists .com/cookie-run-kingdom-tier-list-and-how-to-download

  6. Uwaelelam Divine says

    Great content.
    Well detailed, explanatory and informative. Thanks for the useful tip. You can also check this:
    Fiber types

  7. Bright says

    Your article is nice and I really want to thank you for sharing this post as it contains a lot of details, keep up this good work.

  8. Sunrise says

    Great post, thank you for sharing it was helpful.

  9. paul says

    I love this update, thank you for always proferring solutions on your blog. see these sites for amazing content.

  10. Uwaelelam Divine says

    Never knew this was on the internet, this was really helpful and it was nice reading it. I will be glad to share it with others.

  11. kevinpietersen says

    Cotton fibers develop in a boll across the cotton seeds. Those bolls want to be harvested through a spindle picker or it’s far first-class to handpick them. The use of cotton for cloth is an idea up to now to prehistoric times; fragments of cotton material dated to the 5th millennium BC were placed withinside the Indus Valley Civilization, in addition to material remnants dated decrease returned to 6000 BC in Peru. Although cultivated because of the reality that antiquity, Cotton fibers grow around the cottonseed. And it is 100% cotton fibers the size of the cotton fiber can be from 0.5 to 2.0 inches. “4” types of cotton fibers – Upland Cotton, Pima & Egyptian cotton, tree cotton, Levant cotton…. Aanya linens make bedding products using these types of cotton, allowing them to make the best quality products.

  12. donald smith says

    If seen in the 21st century, the use of cotton is increasing very fast however if seen, cotton is a great fabric widely used. There are users of clothes made from cotton fibers all over the world. Cotton fibers are used not only in the form of clothes. So in the field of medicine too many things started being done, Cotton fibers grow around the cottonseed. And it is 100%
    cotton fibers
    the size of the cotton fiber can be from 0.5 to 2.0 inches. “4” types of Cotton fibers – Upland Cotton, Pima & Egyptian cotton, tree cotton, Levant cotton… Aanya linens make bedding products using these types of cotton, allowing them to make the best quality products.

  13. user says

    How might strength or flexibility be altered if you changed the time when cellulose was added?

  14. Arpine Molasyan says

    hello, can you give me information about 100% cotton muslin fabric shrinkage rate. Thanks

  15. Soham Pratap says

    Nice Article on cotton Even I found this following guide –goo.gl/YuGZfn Anyhow thank you for your useful information.

  16. chris says

    hey I have a question and i was hoping you could help. I work with patients in wound care and lymphedema. I use “Comprilan” and “Rosidal k” a lot for my patients. These bandages advertise 100% cotton but seem to have incredible elastomeric properties What material allows this elasticity? How can this be 100% cotton.??????

    1. KT says

      As such cotton does have high elasticity not more than 10%. If the fabric is getting stretched more than that but around 20% it can with modified fabric and yarn construction like higher twist in yarn. If suppose elasticity is further more, then it can be other fibre like Nylon (one man made fibre). In case of cotton fabric elasticity is enhanced around 30 to 200% with the addition of Lycra filament (ranging 4-10% by weight) during fabric or yarn manufacturing. This you can see in socks, elastic knitted fabric and cotton stretchable elastic jeans. In that case it is specificaly mentioned Lycra % on fabric garment. In such fabric if you open yarn from fabric you will find very tinny white filament i.e Lycra filament (like synthetic rubber- 3-4 time elasticity).

    2. Srabon says

      You can check if it 100% cotton or not by burn test