Yarn Formation Techniques

The Fibre formation process includes a change in shape, structure, and properties of the thermoplastic polymer. The polymer pellets or granules are fed into an extruder where, through heating, their melting temperature is exceeded. The polymeric melt is then transported, under pressure, to the spinneret. Yarn formation methods were originally developed for spinning of natural fibers including cotton, linen, wool and silk.

Yarn Formation Techniques Read More »