Common fabric defects and its causes
Common Defects of Fabrics during manufacturing process includes back fabric seam impression, birds eye, bowing, broken colour pattern, colour out, colour smears, crease mark, drop stitching, dye streak in printing, hole, jerk in, knots, mixed yarn, mottled, needle line, open reed, pin holes, press off etc.