Breathable Fabrics

Home » Breathable Fabrics
breathable-cotton-fabric

Study on application of reduced Graphene Oxide on cotton fabric for Breathable Waterproof finish

This article explains the application of reduced graphene oxide on cotton woven fabric to achieve breathable waterproof finishing. After finishing the fabric was analysed various morphological properties as well as physical properties to confirm comfortability.

Study on application of reduced Graphene Oxide on cotton fabric for Breathable Waterproof finish Read More »

water-repellent-leaf

Introduction to breathable water-repellent textiles and their production methods

Breathability refers to the ability of a fabric to absorb moisture and release it through the material itself, allowing it to ‘breathe’. Breathable Fabrics transmit body moisture away from the body, thus maximizing comfort and dryness during outdoor activities.

Introduction to breathable water-repellent textiles and their production methods Read More »