ISO 1833-18
Textiles — Quantitative chemical analysis — Part 18: Mixtures of silk with wool or other animal hair (method using sulfuric acid)
Silk dissolved in sulfuric acid, leaving wool or other animal hair. Two protein fibres separated on their different resistance to acid - a narrow margin, and the reason…