A blended fabric is a fabric woven or knitted from yarns in which two or more kinds of fibre are mixed, such as polyester and cotton, so that every yarn carries both. Blending gives one cloth properties no single fibre has: polyester/cotton, the most common blend, takes strength, crease resistance and quick drying from the polyester and absorbency and comfort from the cotton, and costs less than all-cotton cloth. The mix is stated as a ratio by weight, such as 65/35 (65% polyester, 35% cotton), and the label must list every fibre by its percentage of the fibre weight. A fabric that uses one fibre in the warp and another in the weft, without mixing them in the yarn, is a mixed or union fabric rather than a blend. The trade-offs are pills that stay on the surface, two dye classes in one fabric, an iron set for the more heat-sensitive fibre, and cloth that is hard to recycle back into fibre.
Last verified: 18 November 2026. Labelling rules are quoted from the US Code of Federal Regulations and EU Regulation 1007/2011, customs rules from the World Customs Organization’s Harmonized System, moisture allowances from the EU regulation, and prices from the site’s own exchange series. Every source is linked where it is used and listed at the end.
Blended fabric at a glance
| Question | Short answer | Section |
|---|---|---|
| What does blended fabric mean? | A fabric whose yarns each contain two or more fibres, mixed before or during spinning | What is a blended fabric |
| Blended or mixed fabric? | Blended: fibres mixed inside every yarn. Mixed or union: different yarns, for example cotton warp and linen weft | Blended, mixed and union |
| Why blend? | To combine properties, lower cost, make colour effects and help processing | Advantages |
| What are the drawbacks? | Pilling, two dye classes, ironing limited by the weaker fibre, hard to recycle | Disadvantages |
| Which blends are common? | Polyester/cotton, polyester/viscose, wool/polyester, viscose/cotton, cotton/elastane | Common blends |
| What does 65/35 mean? | 65% of the fibre weight is the first fibre named, 35% the second | Blend ratio |
| What must the label say? | Every fibre with its percentage by weight, largest first; 3 points of tolerance | Labels |
| How is the blend checked? | One fibre is dissolved out of a weighed sample and the rest weighed (ISO 1833) | Testing |
What is a blended fabric?
Blended fabric means a cloth made from blended yarn: the fibres are combined in a set ratio before or during spinning, so each yarn, and therefore every part of the fabric, holds the same mix. The blend is made in the spinning mill, usually by dosing each fibre by weight in the blowroom or by feeding slivers of each fibre together at the draw frame; the site’s guide to fibre blending in spinning works through both. Once the yarn is spun, the fabric can be woven or knitted like any other, so a blend can be a poplin shirt, a twill trouser, a jersey T-shirt or a suiting.
Blends are the normal state of the trade, not an exception. The spinning machine maker Rieter’s market outlook assumes that 55% of staple fibre will be spun into blended yarns and 45% processed pure, and names a mix of cotton and polyester as the most popular blend (Rieter, Unique Solutions for Processing Man-Made Fibers, 2021). Those two fibres also dominate supply: Textile Exchange’s Materials Market Report 2025 put polyester at 59% of all fibre produced in 2024 and cotton at 19% (Textile Exchange).
A blended fabric is neither natural nor synthetic: it is a mixture, and the label says how much of each. “Poly blend” or “polyester blend” means polyester is one of the fibres, usually with cotton or viscose; the label gives the proportions.
Blended, mixed and union fabrics: the difference
- Blended fabric. The fibres are mixed inside each yarn (an intimate blend). A 65/35 polyester/cotton shirting is the standard example.
- Mixed or union fabric. Each yarn is one fibre, but different yarns are combined in the cloth, typically one fibre in the warp and another in the weft (a mixed weave), or alternating yarns in a knit (a mixed knit). EU law names one such cloth: a fabric with a pure cotton warp and a pure flax weft, in which flax is at least 40% of the weight of the unsized fabric, may be sold as “cotton linen union”, with the specification “pure cotton warp, pure flax (or linen) weft” (Regulation (EU) No 1007/2011, Article 9(3)).
- Core-spun and plied yarns. Some yarns combine fibres without mixing them: a core-spun yarn wraps cotton round a continuous elastane filament, and a plied yarn twists together strands of different fibres. The fabric still contains two fibres and is labelled as such. The core-spun yarn page shows how the elastane share is worked out.
For the buyer the difference matters less than for the maker: all three are multi-fibre products and carry the same kind of label. It matters in the mill, because a union fabric shows each fibre in its own yarns (one may take dye and the other not), and in customs, where the fibre that predominates by weight decides the tariff heading (below). The site’s older page on blended and mixed fibres classifies the yarn types.
Advantages of blended fabrics: why fibres are blended
- Properties neither fibre has alone. Polyester is the stronger fibre: 46.39 cN/tex against 27.55 cN/tex for the cotton in one blending trial (Hossen and Saha, Tekstilec, 2023). Cotton holds the water: the EU’s moisture allowance for fibre-content calculations is 8.5% for cotton and 1.5% for polyester (Regulation 1007/2011, Annex IX). Blend them and the cloth is stronger and quicker to dry than cotton, and more absorbent and comfortable than polyester. Polyester also resists creasing and holds heat-set pleats, while cotton creases easily (see the polyester and cotton comparison).
- Lower cost. Polyester staple fibre is the cheaper fibre. On the Zhengzhou exchange on 6 November 2026, cotton settled at 15,345 CNY a tonne and polyester staple fibre at 7,746 CNY a tonne, about half (cotton price, polyester staple price). The worked example below prices the blend.
- Colour effects. Fibres take different dye classes, so one dyebath can colour one fibre and leave the other white, or two dyes can give two shades: cross-dyed and heather effects. Mélange yarns blend dyed with undyed fibre on purpose.
- Processing. A longer, stronger fibre helps carry a weaker one through spinning and weaving: in rotor spinning of recycled cotton, polyester serves as a supporting fibre (Rieter, 2021).
- Even raw material. Blending many lots of one fibre evens out the variation from bale to bale, which is why even a 100% cotton yarn is blended in the blowroom (why fibres are blended).
Worked example 1: what a 65/35 polyester/cotton mix costs in fibre. At the 6 November 2026 settlements, a tonne of fibre for a 65/35 blend costs 0.65 × 7,746 + 0.35 × 15,345 = 5,034.90 + 5,370.75 = 10,405.65 CNY, against 15,345 CNY for all-cotton: 4,939.35 CNY, or 32%, less. A 50/50 blend costs 11,545.50 CNY. The blend cost solver, opened with these figures, works it the other way round: give it each fibre’s moisture allowance as the property (cotton 8.5, polyester 1.5) and the blend’s 3.95% as the target, and it returns 35% cotton and 65% polyester at 10.41 CNY a kilogram, 10,405.65 CNY for 1,000 kg and 4.94 CNY a kilogram saved against cotton alone. These are fibre prices only: spinning, waste and the extra dyeing step are not in them, and both prices move daily, so read the series rather than one day’s number.
Disadvantages of blended fabrics
- Pills that stay. Rubbing rolls loose fibre ends into small balls. With a weak fibre they break away; with polyester they do not: as the fibre maker Trevira put it in a patent, “owing to the high strength of polyester fibers, these balls or pills cannot drop off, but remain on the surface” (US 7,189,794 B2). Spun polyester blends are the classic case; the polyester page covers low-pill grades and the test.
- Two dye classes. Each fibre needs its own dye: disperse dye for polyester, reactive, vat, sulphur or direct dye for cotton. A polyester/cotton fabric is therefore dyed twice over, in two baths or in one bath in two steps, with polyester dyed at 120 to 140 °C (DyStar, US 5,693,103). The textile dyeing page sets out the routes.
- Ironing set by the weaker fibre. Polyester softens and melts at 250 to 260 °C. The care-label iron with two dots means a sole plate of at most 160 °C, which GINETEX equates with the “wool/silk/polyester/viscose” setting; three dots, 210 °C, is the cotton and linen setting (GINETEX care symbols). A polyester/cotton shirt is ironed at the polyester setting, not the cotton one.
- Hard to recycle. A cotton-polyester or cotton-elastane garment cannot be separated by mechanical tearing, and Textile Exchange describes recycling fibre from blended textiles as a significant challenge (see recycling post-consumer fibre).
- A compromise. A blend is less absorbent than cotton and weaker than polyester; it does not reach the best of either fibre in any one property. Which side to favour is the choice the blend ratio makes.
Common blended fabrics and what each fibre brings
The table lists the blends a buyer meets most often. The middle column is what each fibre contributes; the moisture column is the blend’s agreed allowance under EU Regulation 1007/2011 (Annex IX), worked from each fibre’s figure for the example ratio. It is the figure a laboratory adds to dry fibre mass when it checks a label, a fair guide to how much water each blend holds compared with the others. The last column is the standard that measures the blend.
| Blend | What each fibre brings | Moisture allowance, example ratio | Content test |
|---|---|---|---|
| Polyester/cotton (polycotton) | Polyester: strength, crease resistance, quick drying. Cotton: absorbency, comfort, a natural feel | 65/35: 3.95%. 50/50: 5.00%. Cotton alone: 8.50% | ISO 1833-11 |
| Polyester/viscose | Polyester: strength and shape. Viscose: absorbency, soft drape, bright colour | 65/35: 5.53% | ISO 1833-11 |
| Wool/polyester | Wool: warmth, resilience, drape. Polyester: strength, crease and press retention, lower cost | 50/50 (combed wool): 9.88% | ISO 1833-4 |
| Viscose/cotton | Both cellulosic and absorbent; viscose adds softness and lustre | 50/50: 10.75% | ISO 1833-6 |
| Cotton/elastane (stretch cotton) | Cotton: the fabric. Elastane: stretch and recovery from a small share | 95/5: 8.15% | ISO 1833-20 |
| Cotton/linen (often a union) | Linen: crisp handle and coolness. Cotton: softness and lower cost | 60/40: 9.90% | by warp and weft, or chemically |
Allowances used: polyester and elastane 1.50%, cotton 8.50%, viscose 13.00%, flax 12.00%, combed wool 18.25% (Annex IX). The fibre properties are set out, with their sources, on the site’s pages on polyester, cotton, viscose, wool, linen and spandex, whose section on labelling covers labels such as “98% cotton, 2% spandex”. Other blends exist: nylon and acrylic are blended with wool, silk with cotton, and three-fibre blends of polyester, cotton and viscose. A blend of three fibres is analysed under ISO 1833-2.
Blend ratio: what 65/35 and 50/50 mean
A blend ratio is a ratio of weights. “65/35 polyester/cotton” means that in every 100 g of fibre, 65 g is polyester and 35 g cotton. It says nothing about the number of fibres or yarns: polyester is lighter for its volume (1.38 g/cm³ against 1.52 to 1.56 for cotton), so a 50/50 blend holds more polyester than cotton by volume. On a label the larger share comes first, so “60% cotton, 40% polyester” is a cotton-majority blend and “65% polyester, 35% cotton” a polyester-majority one.
Polyester/cotton is made across the range. The research trials cited on this site used 65/35 polyester/cotton (Mamuye and Gedefaw, 2025) and cotton/polyester at 50/50, 60/40 and 70/30 (Hossen and Saha, 2023), and Rieter’s own trials ran from 2% to 67% polyester. More polyester gives a stronger, quicker-drying, more crease-resistant fabric; more cotton gives a softer, more absorbent one. No ratio is right for every use, and none is fixed by a standard. The ratio is set in spinning; how a mill sets it at the draw frame, and what one missing sliver does to it, is worked in the draw frame blend calculator and on the fibre blending page.
Fibre content labels on blended fabric
Both the EU and the US require a blend to be labelled with each fibre’s share of the fibre weight. The rules differ in the detail.
| Rule | European Union (Regulation 1007/2011) | United States (16 CFR Part 303) |
|---|---|---|
| What the label lists | The name and percentage by weight of all constituent fibres, in descending order (Article 9(1)) | Each fibre of 5% or more by its generic name and percentage of the total fibre weight |
| Small shares | A fibre of up to 5%, or fibres totalling up to 15%, may be grouped as “other fibres” with their total percentage, where they cannot easily be stated at manufacture (Article 9(2)) | A fibre under 5% is “other fiber”, unless it has “a clearly established and definite functional significance”, as in “96 percent Acetate, 4 percent Spandex” (303.3(a)) |
| “100%”, “pure”, “all” | Only for products of one fibre; up to 2% of technically unavoidable extraneous fibre allowed, 5% after carding (Article 7) | No tolerance at all when a product is represented as wholly one fibre (303.43(c)) |
| Tolerance between label and test | 3%, in relation to the total weight of fibres (Article 20(3)) | 3 percent of the total fibre weight: a label saying 40% allows 37 to 43% (303.43(a)) |
| Hard-to-state mixtures | “Mixed fibres” or “unspecified textile composition” may be used (Article 9(4)) | Not provided |
| Wool in a blend | “Virgin wool” or “fleece wool” may describe wool in a mixture only if it is at least 25% of the weight and the full composition is given (Article 8(2)) | Wool labelling is under the separate Wool Products Labeling Act |
| Decorative and antistatic fibres | Visible decorative fibres up to 7%, and antistatic or metallic fibres up to 2%, need not be counted (Article 10) | Permissive ornamentation is left out of the fibre content the tolerance applies to (303.43(a)) |
The tolerance is percentage points of the whole fibre weight, not a percentage of the declared figure. Worked example 2: is the label on this blend right? A shirting is labelled “60% cotton, 40% polyester”. A laboratory dissolves the cotton out under ISO 1833-11 and reports 56.4% cotton and 43.6% polyester. Each fibre is 3.6 points from its label, and the band for cotton runs from 57 to 63%, so both fibres are 0.6 points outside it and the label needs correcting. The fibre content tolerance calculator, opened with these figures, shows a margin of −0.60 points with two fibres outside the band. Had the test found 57.5% cotton, the margin would be +0.50 and the label would stand. The US rule adds that a deviation beyond the band is not misbranding if it came wholly from unavoidable variation in manufacture despite due care (303.43(b)); that is a question about the mill, not the arithmetic.
Blended fabric in customs: which fibre decides the tariff
Customs classify woven fabric by the fibre that predominates by weight. The Harmonized System’s rule is that goods of Chapters 50 to 55 made of a mixture of textile materials “are to be classified as if consisting wholly of that one textile material which predominates by weight over any other single textile material”; when no material predominates, the heading that comes last in numerical order is used (HS 2022, Section XI, Note 2(A)). The Harmonized System then has headings written for polyester/cotton blends:
| Woven fabric | HS heading | Why |
|---|---|---|
| 65/35 polyester/cotton, 120 g/m² | 55.13 | Synthetic staple fibres under 85%, mixed mainly or solely with cotton, not over 170 g/m² |
| 65/35 polyester/cotton, 220 g/m² | 55.14 | The same, over 170 g/m² |
| 60/40 cotton/polyester, 150 g/m² | 52.10 | Cotton under 85%, mixed mainly or solely with man-made fibres, not over 200 g/m² |
| 60/40 cotton/polyester, 240 g/m² | 52.11 | The same, over 200 g/m² |
| 50/50 polyester/cotton | 55.13 or 55.14 | Neither fibre predominates, so the later heading, Chapter 55, applies |
Headings and weight limits are from the WCO’s HS 2022 nomenclature, Chapters 52 and 55. Knitted fabrics fall in Chapter 60 instead, and each country adds its own digits and duty rates beyond the six-digit HS code, so a shipment is classified on the importing country’s tariff. What the table shows is that a blend ratio near 50/50 can change the heading, and with it the duty, which is one more reason the ratio is tested rather than assumed. Grams per square metre come from the fabric GSM calculator or a weighed sample.
How the blend in a fabric is tested
First the fibres are identified, by microscope and chemical tests (ISO/TR 11827); the microscopic appearance of fibres page shows what each looks like. Then the proportions are measured: a weighed, dried sample is treated with a reagent that dissolves one fibre, and the residue is washed, dried and weighed. ISO 1833-1 sets the common procedure, and each later part covers a pair of fibres: ISO 1833-11 dissolves cotton or viscose in sulfuric acid to leave polyester; ISO 1833-4 dissolves wool in hypochlorite; ISO 1833-20 dissolves elastane. The EU’s official methods in Annex VIII of Regulation 1007/2011 work the same way. The result is expressed on dry mass plus each fibre’s agreed allowance, which is why a contract and a label should name the basis.
Worked example 3: the blend’s allowance on an invoice. Yarn and cloth are often sold at a commercial weight: oven-dry mass plus the agreed allowance. For a 65/35 polyester/cotton blend the allowance is 0.65 × 1.5 + 0.35 × 8.5 = 3.95%. A 1,000 kg lot found to hold 4.5% moisture on its dry weight is 1,000 ÷ 1.045 = 956.94 kg dry, and 956.94 × 1.0395 = 994.74 kg at commercial weight: 5.26 kg of water the buyer should not pay for. The blend invoice weight calculator, with these figures, shows the same. The moisture regain calculator converts between regain and moisture content.
How to wash and care for blended fabrics
- Follow the label, not the fibre. GINETEX, which administers the care symbols of ISO 3758, says the washing temperature “must be selected solely on the basis of the care label and not according to the fibre content”. The label is written for the whole garment, with both fibres, its dyes and its trims.
- Iron for the more sensitive fibre. For polyester blends that is two dots, 160 °C at most: a hot cotton setting can glaze or melt the polyester.
- Expect less shrinkage than cotton, not none. Heat-set polyester does not shrink at its label temperature; the cotton or viscose in the blend can. Dimensional change in washing is measured by ISO 5077.
- Expect pills to stay. On a spun polyester blend the pills do not fall away on their own, so they have to be removed; less rubbing in the wash means fewer of them.
Questions about blended fabrics
What does blended fabric mean?
A fabric made of yarn in which two or more fibres are mixed, such as polyester and cotton. The label states each fibre’s share of the weight, largest first.
What are examples of blended fabrics?
Polycotton shirting and sheeting (polyester/cotton), polyester/viscose suiting, wool/polyester suiting, stretch denim and stretch chinos (cotton/elastane), and viscose/cotton dress fabric.
What is the difference between blended and mixed fabric?
In a blended fabric the fibres are mixed inside each yarn. In a mixed or union fabric each yarn is a single fibre and different yarns are combined, for example a cotton warp with a linen weft. Both are labelled with their fibre percentages.
Is blended fabric good?
For everyday wear, often yes: polyester/cotton is stronger, dries faster, creases less and costs less than cotton, and is more comfortable than polyester. It pills more than cotton, is ironed at a lower setting and is harder to recycle. For the most absorbent cloth, choose more cotton; for the hardest-wearing, more polyester.
What does poly blend fabric mean?
A blend that contains polyester, usually with cotton or viscose. “Poly-cotton” or “polycotton” is polyester with cotton; the label gives the ratio, for example 65% polyester, 35% cotton.
Is blended fabric natural or synthetic?
Neither: it is a mixture. A polyester/cotton fabric is part synthetic and part natural, in the proportions on the label. A viscose/cotton blend is all cellulose, but viscose is a man-made fibre.
Does blended fabric shrink?
Less than cotton of the same construction, because heat-set polyester does not shrink at its label temperature, but the cotton or viscose share can. Wash at the temperature on the care label.
How do I know what a blended fabric is made of?
Read the fibre content label, which by law lists every fibre with its percentage. To check it, a laboratory dissolves one fibre out of a weighed sample (ISO 1833) and compares the result with the label, allowing 3 percentage points either way.
Related on this site
- Fibre blending in spinning: where and how mills blend, the draw frame arithmetic, and the faults a poor blend causes.
- Characteristics of blended yarn and fabric and blended fibre analysis: fibre by fibre, and blended against mixed yarns.
- Yarn blending calculations and drafting polyester/viscose blend yarns.
- Types of fabric and types of textile fibres.
- Calculators: blend cost solver, fibre content tolerance, blend invoice weight, draw frame blend, mélange blend ratio, blend homogeneity and bale laydown blend.
Sources
- Regulation (EU) No 1007/2011 on textile fibre names and labelling, consolidated text: Articles 7, 8, 9, 10 and 20, Annexes VIII and IX.
- US Code of Federal Regulations, 16 CFR Part 303 (Textile Fiber Products Identification Act rules): § 303.3, fibres under 5%; § 303.43, fibre content tolerances.
- World Customs Organization, HS Nomenclature 2022: Section XI notes, Chapter 52, Chapter 55.
- Rieter, Unique Solutions for Processing Man-Made Fibers, brochure 3440, 2021.
- Textile Exchange, Materials Market Report 2025.
- J. Hossen and S. K. Saha, Influence of blending method and blending ratio on ring-spun yarn quality: a MANOVA approach, Tekstilec 66(3), 2023, 227–239. W. Mamuye and M. Gedefaw, polyester–cotton blending methods at Buluko Textile, Journal of Engineering, 2025.
- Patents: US 7,189,794 B2 (Trevira, low-pill polyester); US 5,693,103 (DyStar, dyeing polyester/cotton blends).
- GINETEX, care symbols.
- Prices: Zhengzhou Commodity Exchange settlements for cotton (CF701) and polyester staple fibre (PF701), 6 November 2026, as carried in the site’s cotton and polyester staple series.
- Standards, by ISO’s published scope and the site’s register: ISO 1833-1, -2, -4, -6, -11 and -20; ISO/TR 11827; ISO 3758; ISO 5077.
How this page is kept
Last verified: 18 November 2026. The labelling rules, customs headings and moisture allowances are quoted from the regulations and the HS nomenclature themselves. Fibre strengths are from the peer-reviewed trial named, the blending share from the machine maker’s own estimate, and production shares from Textile Exchange. Prices are one day’s settlements and are given with their date. The three worked examples were redone by hand, and each calculator link was opened to check that it shows the figures quoted. Example ratios in the blends table are illustrations, not standard or typical ratios.
Change log. 18 November 2026: rewritten in full as the site’s main page on blended fabrics, and the overlapping article on the advantages of blended fabrics was merged into it. Withdrawn as unsourced: a timeline of blends by decade, workwear and formal-wear uses assigned to particular ratios, tri-blend recipes, claims of “molecular-level” blending (blending is mechanical, fibre by fibre), and generic lists of future trends. The earlier page also suggested that blends need less water, energy and chemicals; no source was found, and a polyester/cotton fabric needs two dyeing steps.
Found an error, or a newer figure? Please tell us through the contact page, naming the section and the source that disagrees.









thanks for giving me this information
can you explain how these fabrics are mixed or blended?
Sure there is plenty of room to improve as you didn’t even hit major fabrics blend… Some of which are Terry Rayon, Cotton Wool etc
NOT INFORMATIVE. NOT CLEAR ENOUGH
How can we improve it? Do you have any suggestions?
Very informative……
Thanks for sharing.