Home » Fabric » Types of Fabric: Names, Pictures and Uses from A to Z

Types of Fabric: Names, Pictures and Uses from A to Z

Fabrics are classified by construction (woven, knitted, nonwoven) and by fibre. An A to Z of 88 fabric types with pictures, fibres, weights and uses.

Edges of folded fabrics stacked in rainbow order, from red, orange and yellow through pink, purple and blue to green and brown

Fabrics are classified in two ways: by construction, which is how the material is held together, and by fibre, which is what it is made of. By construction there are four groups. A woven fabric has two sets of yarns crossing at right angles. A knitted fabric is made of rows of interlocking loops. A nonwoven is a sheet of fibres bonded directly, with no yarn at all; felt is one. The fourth, smaller group covers everything else: lace, nets, braids and tufted fabrics. By fibre, a fabric is natural (cotton, linen, wool, silk), man-made from a natural polymer (viscose, lyocell, acetate), synthetic (polyester, nylon, acrylic, elastane), or a blend.

Most fabric names describe a construction and a finish, not a fibre. Chiffon is a sheer plain weave of twisted yarns whether it is silk or polyester; jersey is a plain weft knit whether it is cotton or viscose; denim is a twill with a dyed warp. That is why the table below gives construction and fibre in separate columns. It lists 88 fabrics from A to Z, each with its construction, the fibres it is usually made from, its weight or feel, and its uses. A description of most of them follows, with a picture and a note on how to recognise each, and the original list of 87 is in a printable PDF with pictures.

Last verified: 5 October 2026. Sources are linked where they are used and listed at the end.

Types of fabric from A to Z

Each name links to its picture and description further down the page; each construction has a page of its own too, for woven, knitted and non-woven fabrics. In the weight column, sheer means you can see through it, light means a blouse or shirt weight, medium a trouser or furnishing weight, and heavy a coat, bag or upholstery weight. Figures are given only where a mill, a standard or a textile glossary publishes them; silk is sold by the momme, a Japanese unit equal to about 4.3 g/m², and the weight section explains grams per square metre and ounces.

FabricConstructionTypical fibreWeight or handTypical uses
AertexWoven, cellular (leno-type)CottonLight, openSports and school shirts
Aida clothWoven, even-weave gridCottonStiff, open gridCross-stitch embroidery
BaizeWoven, nappedWool, cottonDense, felt-like napCard and gaming tables, notice boards
BatisteWoven, plain, fineCotton, polyester-cottonSheer, very light, softLingerie, nightwear, linings, handkerchiefs
Bird’s eyeWoven dobby pattern, or a knit backingCotton, variousLight to mediumNappies (historically); patterned knits
BombazineWoven, twillSilk warp, worsted weftMedium, dullHistoric dress and mourning wear
BroadclothWoven, plain, fine crosswise ribCotton, polyester-cottonLight to medium, lustrousShirts
BrocadeWoven, Jacquard, raised figuresSilk, metallic yarn, syntheticsMedium to heavySaris, evening wear, upholstery
BuckramWoven, open, stiffenedCotton, linenStiffInterlinings, hats, bookbinding
Cable knitWeft knit, loops crossedWool, acrylicHeavy, bulkySweaters
CalicoWoven, plainCottonMediumDresses, quilts, toiles, bags
CambricWoven, plain, calenderedCotton, linenLight, smooth, slight glossHandkerchiefs, shirts, linings
Canvas and duckWoven, plain, compactCotton, linen, syntheticsHeavy: about 200 to 1,700 g/m² (6 to 50 oz/yd²)Tents, bags, shoes, sails, artists’ canvas
CasementA use: curtain clothCotton, blendsSheer to mediumCurtains
ChambrayWoven, plain, coloured warp, white weftCottonLight; nearly square, e.g. 80 × 76 threads per inchShirts, dresses; heavier grades for workwear
CharmeuseWoven, satinSilk, polyesterLight, fluid; silk from about 12 mommeLingerie, blouses, evening wear
CheeseclothWoven, low-count plainCottonVery light, looseKitchen and dairy use, summer clothes
ChenilleWoven or knitted from chenille yarnCotton, viscose, acrylic, polyesterSoft, fuzzy pileUpholstery, throws, bathrobes
CheviotWoven, twill (a tweed)WoolMedium to heavy, harshSuits, coats
ChiffonWoven, plain, highly twisted yarnsSilk, polyester, nylonSheer; silk about 6 to 10 mommeEvening wear, scarves, overlays
ChinoWoven, twillCotton, cotton blendsMedium, smoothTrousers, summer uniforms
ChintzWoven, plain, printed and glazedCottonMedium, glazedCurtains, upholstery
CorduroyWoven, cut weft pile in lengthwise cordsCottonMedium to heavy; 5 to 16 cords per inchTrousers, jackets
CrepeWoven or knitted; twisted yarns, crepe weave or finishSilk, wool, viscose, polyesterLight, pebblyDresses, blouses
Crepe de chineWoven, plain, crepe-twisted weftSilk, polyesterLight, softBlouses, dresses, scarves
CrewelWool embroidery on a woven groundWool on cotton or linenMedium to heavyCurtains, cushions, bedcovers
DamaskWoven, Jacquard, reversible satin figureLinen, cotton, silkMedium, flat, glossyTable linen, furnishings
DenimWoven, 2/1 or 3/1 twill, coloured warpCotton, cotton-elastaneMedium to heavyJeans, jackets, workwear
DimityWoven, plain, often corded stripesCottonSheer, thinSummer dresses, babywear, curtains
Double knitWeft knit, two needle bedsPolyester, wool, cottonMedium, stableDresses, trousers
DrillWoven, 2/1 twillCottonMedium to heavy, firmUniforms, workwear, pocketing
FeltNonwoven (matted or needled); also fulled woven woolWool, syntheticsVaries; no grainHats, crafts, insulation
FlannelWoven, plain or twill, nappedWool, cottonMedium, softSuits, shirts, nightwear, sheets
FleeceKnitted (sometimes woven), napped or pilePolyester, cottonLight to heavy; polar fleece in 100, 200 and 300 weightsSweatshirts, jackets
FoulardWoven, 2/2 twill, printedSilk, polyester, acetateLight, lustrousTies, scarves
French terryWeft knit, loops on the backCotton, cotton-polyesterMedium, softSweatshirts, joggers
FustianWoven, heavy, often cut weft pileCotton (historically linen warp)HeavyWorkwear
GabardineWoven, warp-faced twill (45° or 63°)Worsted wool, cotton, polyesterMedium, firmSuits, trousers, raincoats
GauzeWoven, gauze (leno) or loose plainCotton, silk, syntheticsVery light, openDressings, curtains
GeorgetteWoven, plain, crepe yarns both waysSilk, polyesterSheer, grainySaris, blouses, dresses
GinghamWoven, plain, yarn-dyed checksCotton, cotton blendsLight to mediumShirts, dresses, tablecloths
Glass fabricWoven from glass filament yarnGlassMedium to heavyFire blankets, insulation, composites
IntarsiaWeft knit, colour blocksWool, acrylicMediumSweaters, socks
InterlockWeft knit, double (crossed 1×1 rib)CottonMedium, smooth both sidesT-shirts, polo shirts, babywear
Jacquard knitWeft knit, needle-selected patternWool, acrylic, cottonMediumSweaters
Jersey (single)Weft knit, plain stitchCotton, viscose, polyester, elastaneLight; two common T-shirts use 145 and about 180 g/m²T-shirts, underwear, dresses
Kashmir silkWoven, plain, embroidered or printedSilkLightSaris, shirts, stoles
KhadiHand-woven from hand-spun yarnCotton, silk, woolVaries, slightly unevenShirts, kurtas, furnishings
KhakiA colour; usually drill or twillCotton, wool, blendsMediumUniforms, workwear
LaceOpenwork, by hand or machineCotton, nylon, polyesterLight, openLingerie, bridal wear, trims
LaméWoven (or knitted) with flat metallic threadsMetallic yarn with silk or syntheticsLight to medium, metallicEvening wear, costumes
LawnWoven, plain, fineCotton, linenLight, crispBlouses, handkerchiefs, nightwear
LenoWoven, paired twisting warp endsCotton, syntheticsOpen, stableCurtains, nets, produce sacks
Linsey-woolseyWovenLinen warp, wool weftCoarse, sturdyHistoric clothing and bed covers
MadrasWoven, plain, yarn-dyed checks and plaidsCottonLightSummer shirts, shorts
Madras muslinWoven gauze with cut extra-weft figuresCottonSheerCurtains
MoleskinWoven, heavy sateen, napped and shearedCottonHeavy, suede-likeTrousers, workwear
MousselineWoven, plain, very fineSilk, wool, cottonSheer, lightDresses, scarves
MuslinWoven, plainCotton, polyester-cottonSheer to mediumDresses, toiles, kitchen use
Net and tulleKnotted or machine-made mesh; tulle has a hexagonal meshNylon, polyester, silk, cottonVery light, openVeils, ballet costumes, curtains
OrgandyWoven, plain, chemically stiffenedCottonSheer, stiff, wiryCollars, trims, curtains
OrganzaWoven, plain, filamentSilk, polyester, nylonSheer, stiff; silk about 5 to 7.5 mommeBridal and evening wear, overlays
OxfordWoven, modified basketCotton, polyester-cottonMedium, softShirts
PercaleWoven, plain, closeCotton, polyester-cottonCrisp, matt; 80 × 80 threads per inch or moreSheets, dresses
PointelleWeft knit with transferred-loop eyeletsCotton, viscoseLight, lacyTops, babywear
PoplinWoven, plain, more ends than picksCotton, polyester-cottonLight to medium, fine ribShirts, dresses
PurlWeft knit, courses alternate face and backWool, acrylicThickSweaters, children’s wear
RaschelWarp knitNylon, polyester, cottonLight to heavy, often openLace, power mesh, nets
RibWeft knit, wales alternate face and backCotton, cotton-elastane, woolVery elastic across the widthCuffs, collars, waistbands, fitted tops
SateenWoven, satin weaveCottonSmooth, lustrousSheets
SatinWoven, satin weaveSilk, acetate, polyesterSmooth, lustrousEvening wear, linings
SeersuckerWoven, plain; slack and tight warp stripesCotton, syntheticsLight, crinkled stripesSummer suits, shirts, dresses
SergeWoven, 2/2 twill, smooth faceWorsted woolMedium, firmSuits, uniforms
ShantungWoven, plain, slubbed yarnSilkMedium, crispBridal and evening wear, furnishings
SheetingA use: wide plain or twill clothCotton, polyester-cotton, linenMediumBed sheets
Sliver knitWeft knit with a fibre-sliver pileAcrylic, modacrylicHeavy, long pileImitation fur, linings
TaffetaWoven, plain, fine crosswise ribSilk, acetate, nylon, polyesterCrisp, rustlingEvening wear, linings
TartanWoven, usually 2/2 twill, coloured settWoolMediumKilts, scarves, skirts
TerryWoven, uncut loop pileCotton, cotton blendsMedium to heavy, absorbentTowels, bathrobes
TickingWoven, close (plain, twill or satin)Cotton, linenHeavy, denseMattress and pillow covers
TissueWoven, plain, with zariSilk, synthetics, metallic yarnLight, metallic sheenSaris
TricotWarp knitNylon, polyester, acetateLight, smoothLingerie, linings, sportswear
TweedWoven, 2/2 twill, woollen yarnsWool, wool blendsHeavy, roughJackets, coats, suits
VelourWoven or knitted, short thick pileCotton, wool, polyesterSoft, plushCoats, upholstery, leisurewear
VelvetWoven, cut warp pileSilk, viscose, cotton, polyesterMedium, dense pileEvening wear, upholstery
VelveteenWoven, short cut weft pileCottonMedium, low pileJackets, trousers, dresses
VoileWoven, plainCotton, polyesterSheer, light, softBlouses, sheer curtains
WhipcordWoven, very steep twill with cordsWorsted, wool blends, cottonHeavy, firmUniforms, riding breeches

How to tell woven, knitted and nonwoven fabric apart

Four checks settle the construction of almost any piece of cloth in a minute, with nothing more than a pair of scissors and a magnifier. A counting glass, the small folding lens sold for counting threads, makes the third check easier. Each construction has its own page on this site: woven fabric types, knitted fabric types and non-woven fabrics. When the fibre matters too, the fibre identification tests, including the burn test, are the next step.

CheckWovenKnittedNonwoven
Pull a thread from a cut edgeStraight yarns pull out in two directions at right angles, and the edge fraysA weft knit unravels as one crinkled, looped yarn; a cut edge may curl or ladderThere is no yarn to pull; the edge shows loose fibres or fused filaments
Stretch itLittle give along or across the cloth, more on the diagonal, unless the yarn contains elastaneStretches readily, most of all across the width, and recoversUsually little stretch; it tears or distorts rather than springing back
Look through a magnifierA grid of yarns passing over and under one anotherColumns of V-shaped loops on the face and rows of arcs on the backA random web of fibres, often with a pattern of small bond points
Check the edges of the rollA firm selvedge on both edgesA tube from a circular machine, or slit edgesSlit edges

Woven fabrics

A woven fabric is made on a loom from two sets of yarns: the warp, which runs along the length of the cloth, and the weft, which crosses it. The order in which they pass over and under each other is the weave. ISO 3572 defines the general terms and the three basic weaves. In a plain weave every weft passes over one warp and under the next, which gives the firmest interlacing: poplin, voile, chiffon, taffeta and canvas are plain weaves. A twill steps the interlacing along by one thread on each pick, which draws diagonal lines across the face: denim, drill, gabardine and serge are twills. A satin spaces the interlacings so far apart that long floats of one set of yarns cover the face, which gives the lustre of satin and sateen. Almost every other woven fabric is one of these three with something added: a pile (velvet, corduroy, terry), a figure woven by a Jacquard or dobby mechanism (damask, brocade), crossed warp ends (leno and gauze), or a coloured pattern from dyed yarns (gingham, madras, tartan). The classification of weave patterns covers the derived weaves, and woven fabric types shows the common woven fabrics with pictures.

Knitted fabrics

A knitted fabric is made of loops pulled through loops. The vertical columns of loops are wales and the horizontal rows are courses. In weft knitting, the kind used for most T-shirts, sweaters and sportswear, each course is formed by a yarn running across the fabric, so one yarn can make the whole piece. Its four basic structures are single jersey, rib, interlock and purl. In warp knitting each wale has its own yarn, fed from a beam, and the yarns zigzag between neighbouring wales; tricot and raschel are the two main families, used for lingerie, sportswear linings, lace and nets. A warp knit does not unravel the way a weft knit does. The terms are standardised in ISO 8388, the vocabulary of knitted fabric types. Knitted fabric types describes each structure, from single jersey to raschel, with pictures; the principles of weft and warp knitting and warp knitting have their own articles.

Nonwoven fabrics

A nonwoven skips the yarn altogether: fibres or continuous filaments are laid into a web and bonded by heat, by entangling them with needles or water jets, or with a binder. ISO 9092 sets the definition. Most nonwovens are named after the process that made them: spunbond, meltblown, needle-punched, spunlace (hydroentangled), thermal-bonded, airlaid and wet-laid. Wool felt, made by matting wool fibres with heat, moisture and agitation, is a nonwoven too, and so is flash-spun Tyvek. The non-woven fabrics page explains each process, with worked calculators.

Other constructions

A few fabrics are made in none of the three ways. Lace is an openwork of twisted, looped or knotted threads, made by hand with bobbins or needles, or by machine; much machine lace is now warp-knitted on raschel machines. Nets are knotted, twisted (bobbinet) or warp-knitted. Braids are made by interlacing yarns diagonally, and narrow braids, tapes and webbings have their own article, narrow fabrics. Tufted fabrics, which include many carpets, are made by needling pile yarn into a backing that already exists. Coated and laminated fabrics join a fabric to a film, foam or second fabric, and are covered in coated and laminated textile fabrics.

Types of fabric by fibre

The second way to classify a fabric is by the fibre it is made from. Fibres come from plants, from animals, from natural polymers that are dissolved and spun again, from synthetic polymers, or from minerals. A few fabrics are named after their fibre (linen, silk, wool, cotton), but most fabric names say nothing about it, which is why the law in many countries requires a separate fibre label. In the European Union, Regulation (EU) No 1007/2011 allows only the fibre names in its Annex I on labels and requires each fibre to be listed with its percentage by weight; the generic names of man-made fibres are standardised in ISO 2076. Two fibres dominate by volume: Textile Exchange’s Materials Market Report 2025 put polyester at 59% of all fibre produced in 2024 and cotton at 19%. The full list of fibres, with their sources, is in types of textile fibres.

Fibre groupMain fibresFabrics often made from them
Plant (cellulose)Cotton, linen (flax), hemp, jute, ramieCalico, poplin, denim, lawn, voile, canvas, terry, damask table linen, hessian
Animal (protein)Wool, cashmere, mohair, alpaca, silkFlannel, gabardine, serge, tweed, baize, felt; chiffon, organza, taffeta, charmeuse, shantung
Man-made from natural polymersViscose (rayon), modal and lyocell, acetateCrepe, linings, satin, velvet, jersey
SyntheticPolyester, nylon (polyamide), acrylic, elastane (spandex), polypropyleneGeorgette, satin, taffeta, fleece, tricot, knitwear, stretch denim, spunbond nonwovens
Mineral and other inorganicGlass, carbon, metalGlass and carbon fabrics for composites, filtration and insulation; metallic yarn in lamé and zari
BlendsTwo or more of the abovePolyester-cotton shirting and sheeting, cotton-elastane denim, wool-polyester suiting; see blended fabrics

Measuring a fabric: weight, threads and cover

Two fabrics with the same name can differ a great deal, so a mill specification gives numbers as well: the weight, the number of threads per unit length, and the yarn counts. Several of this site’s calculators work with exactly those numbers. Each link below opens the calculator with the example’s figures already entered.

Fabric weight: GSM and ounces

Fabric weight is the mass per unit area, given in grams per square metre (g/m², usually called GSM) or, in the United States, in ounces per square yard. It is measured by cutting specimens of known area and weighing them, by the methods in ISO 3801 and ASTM D3776. The two units are linked by one exact constant: an ounce is 28.349523 g and a square yard is 0.83612736 m², so 1 oz/yd² is 33.906 g/m². Weight per square metre does not depend on width, but the weight of a running metre does, and that is the figure that sets the price of a roll. A 180 g/m² fabric is 5.31 oz/yd², and at 150 cm wide every running metre weighs 270 g. Open the fabric weight converter with these figures; it is also below, live.

Ends and picks, and the weight they predict

In a woven fabric the warp threads are called ends and the weft threads picks. Counting them per inch or per centimetre, as ISO 7211-2 describes, is the first step in describing a construction. A construction is written as yarn counts and thread counts: 40s × 40s, 133 × 72, for example, means warp and weft yarns of 40 English cotton count (Ne), with 133 ends and 72 picks per inch. Take that as a cotton poplin, a cloth with many more ends than picks, which is what gives poplin its fine crosswise rib. Entered with 6% warp crimp and 4% weft crimp, which are assumptions rather than measurements, the fabric GSM calculator gives a loom-state weight of 125.5 g/m². Loom state means as it comes off the loom: finishing shrinks, washes and sometimes coats the cloth, so the finished weight is different. To go the other way, from a swatch you have weighed and counted to the yarn counts that must have made it, use woven fabric reverse engineering.

Cover factor: how closely a cloth is woven

The thread count alone does not say how closely woven a fabric is, because a thick yarn covers more area than a thin one. Peirce’s cover factor corrects for that: in English units it divides the threads per inch by the square root of the cotton count, and a value of 28 means the yarns touch. For the same 40s poplin the cover factor calculator gives a warp cover of 21.0, a weft cover of 11.4 and a fabric cover of 23.9, so yarn covers about 85% of the area. Weave the same yarn at 60 ends and 56 picks, an open cheesecloth-like sett chosen here only for comparison, and the fabric cover falls to 15.3, about 55%. That is the difference you see when you hold a cheesecloth and a poplin up to the light. The maximum sett calculator gives the other limit: the most ends or picks per inch a weave can take at a given count before the cloth jams.

The weight of a knitted fabric

A knitted fabric has no ends and picks. Its weight follows from the number of loops in a square metre (courses times wales) and the length of yarn in each loop, the stitch length. The knitted GSM calculator opens here with its own default case: 42 courses and 32 wales per inch, a 2.9 mm stitch and a 30s cotton yarn, which give 118.9 g/m². That is about 2.08 million loops and 6 km of yarn in every square metre. The article on calculating GSM for knit fabrics works through the same arithmetic by hand, and the stitch length calculator starts from the machine side.

Pictures of fabric types, A to Z

The pictures show examples, and the note with each says how to recognise the fabric. Weaves are easiest to see with a magnifier on the reverse side, where finishes and prints do not hide them.

Aertex

Aertex Fabric

A cellular cotton cloth: an open, leno-type weave whose small cells trap air. Harmuth’s 1915 dictionary describes English cellular cloth as an open cotton leno used for underwear. Aertex is the brand name of the Cellular Clothing Company, set up in Britain in 1888, and the cloth is still used for sports and school shirts.

Aida cloth

Aida Fabric

An even-weave cotton in which groups of warp and weft threads are woven together to leave a stiff grid of regular holes. Embroiderers work cross stitch over the squares, and Aida is sold by the number of squares per inch.

Baize

baize-fabric

A coarse woollen cloth with a nap on one side, later also made in cotton, so the weave is hidden under a felt-like surface. It is used chiefly to cover card and gaming tables, and for notice boards.

Batiste

Batiste Fabric

A sheer, very fine plain weave, usually of mercerised combed cotton or polyester-cotton, soft to the touch. It is used for lingerie, nightwear, christening gowns, handkerchiefs and linings. The name is traditionally said to come from Baptiste, a weaver of Cambrai, but that is a legend, not a record.

Bird’s eye

birds-eye-knit

The name has two meanings. In weaving, birdseye is a small dobby pattern of diamonds with a dot in the centre, once the standard absorbent cotton for nappies. In knitting, it is the speckled effect on the back of a patterned double knit, produced by the different colours used in the face design. Ask a supplier which one is meant.

Bombazine

Bombazine Fabric

A twilled or corded dress fabric made with a silk warp and a worsted wool weft, dull rather than lustrous. Black bombazine was widely used for mourning dress in the nineteenth century.

Brocade

Benaras_brocade_sari
By Anilbhardwajnoida (Own work) [ CC BY-SA 3.0], via Wikimedia Commons

A rich Jacquard-woven fabric with raised figures or flowers over its whole surface, often with gold or silver threads, on a satin or twill ground. The Banarasi saris of Varanasi, India, are among the best-known brocades. See also brocade for upholstery.

Buckram

Buckram Fabric

A coarse, open cotton or linen cloth stiffened with glue or heavy size. It is used as an interlining in collars, cuffs and waistbands, in bookbinding, for hat shapes and to stiffen curtain headings.

Cable knit

cable-knit

A weft knit in which groups of loops are moved across one another so that the wales twist like ropes. Cables are typical of heavy sweaters, usually in wool or acrylic.

Calico

calico-prints

A plain, closely woven, inexpensive cotton. In the United States calico usually means a cotton printed with small figures on a plain background, used for dresses, aprons and quilts; in Britain the name is also used for plain, unbleached cotton. It is named after Calicut, now Kozhikode, in India.

Cambric

Cambric Fabric

A soft, closely woven white cotton or cotton blend, originally linen, calendered on the face to give it a slight gloss. It is used for handkerchiefs, shirts and linings. The name comes from Cambrai in France, where the cloth is said to have been first made.

Canvas and duck

canvas shoes
Canvas Shoes, by Capri23auto

Compact, firm, heavy plain weaves, usually cotton, often from plied yarns; the trade treats canvas and duck as one family, which ranges from about 6 to 50 oz/yd². Numbered duck is graded by a rule set in a 1924 US Bureau of Standards specification: the number is 19 minus the weight in ounces of one yard of 22-inch-wide cloth. No. 10 duck is therefore 14.7 oz/yd², about 499 g/m². Canvas is used for tents, bags, shoes, sails and as artists’ canvas.

Casement

Casement Fabric

A curtain fabric, named after the casement window. In American usage casement cloth means light, sheer curtain and screening fabrics; the name is also used for heavier cotton and blended curtain cloths like the one pictured. It describes a use, not a construction.

Charmeuse

Charmeuse Fabric

A light, fluid satin-weave fabric with a lustrous face and a dull back, traditionally silk and now often polyester. Silk charmeuse is sold in weights from about 12 momme upwards. It is used for lingerie, blouses and evening dresses.

Cheesecloth

cheese-fabric

A soft, low-count plain weave of cotton, so loosely woven that it is also called gauze. It was first used for wrapping and draining cheese, and is still used in kitchens and dairies and for light summer clothing.

Chenille

Chenille Fabric

A fabric woven, or knitted, from chenille yarn, which has a fuzzy pile standing out on all sides. The yarn itself is cut from a specially woven fabric. Chenille is French for a caterpillar, a name given for the yarn’s furry look. It is used for upholstery, throws, cushions and bathrobes.

Cheviot

Cheviot Fabric

A rugged tweed made from uneven yarn, with a rather harsh hand. It was originally an all-wool twill made from the wool of Cheviot sheep and is used for suits and coats. The picture shows a herringbone twill.

Chiffon

chiffon fabric

A sheer, transparent, very light plain weave made from fine, highly twisted yarns, usually with about the same number and count of threads in warp and weft. Silk chiffon is the original and is sold at about 6 to 10 momme; polyester and nylon chiffon are now more common. The name comes from the French chiffe, a rag or piece of cloth.

Chino

Chino Fabric

A cotton or cotton-blend twill, long used by armies for summer-weight uniforms and often dyed khaki. Today it is mainly a trouser fabric, lighter and smoother than drill or denim.

Chintz

chintz-fabric

A plain-woven cotton printed with bold patterns, usually flowers, and glazed by friction calendering, which gives it a shine; unglazed, the same cloth is called cretonne. It is a furnishing fabric for curtains and upholstery. The name comes from the Hindi chint, from a Sanskrit word for variegated or bright.

Corduroy

Corduroy-Fabric

A weft-pile fabric with ridges of cut pile (cords, or wales) running along its length. Extra weft yarns float over the ground and are cut after weaving, and the cut ends are brushed into rounded cords. It is graded by cords per inch: one British mill’s range runs from 5-wale cord to 16-wale needlecord. The story that the name comes from French corde du roi, the king’s cord, is a folk etymology: the phrase is not found in French.

Crepe

Surface of chirimen (Japanese crepe) which is made of 100% rayon.
By Asanagi(Asanagi (talk)’s file) [CC0],via Wikimedia Commons

A light fabric with a crinkled, pebbly surface, produced in one of four ways: hard-twisted yarns, a chemical treatment, a crepe weave or embossing. In crepe de chine the crepe-twisted yarns are in the weft only; in georgette they are in both directions. The picture shows Japanese chirimen woven from rayon.

Crewel

Crewel Fabric

Crewel is embroidery, not a weave: designs worked in loosely twisted wool yarn on a cotton or linen ground. Crewel work from Kashmir is made for curtains, cushions and bedcovers.

Damask

Damask Fabric

A firm, glossy Jacquard fabric, flatter than brocade and reversible: the figure is woven in satin of one face on a ground of the opposite face, so the pattern shows by the way it catches the light. Linen and cotton damask are the classic table linens; silk and blended damasks are used for furnishings. It is named after Damascus.

Denim

Denim Fabric
Denim Fabric, by Digital Buggu

A firm 2/1 or 3/1 twill with a coloured warp, traditionally indigo, and a white weft, which is why the inside of a pair of jeans is paler. Heavier denims go into jeans and workwear and lighter ones into shirts and dresses; stretch denim adds elastane. The name comes from serge de Nîmes, a cloth from Nîmes in France. The site’s denim fabrics article covers its types.

Dimity

dimity-fabric

A sheer, thin cotton, sometimes with cords or stripes woven in by grouping threads together at intervals. It is used for summer dresses, blouses, babywear and curtains.

Double knit

double-knit

A weft knit made on two needle beds, so both faces show plain loops and the fabric is thicker and more stable than single jersey. It does not curl at the edges. Rib and interlock are both double knits.

Drill

drill-fabric

A strong cotton 2/1 twill, much like denim but usually dyed in the piece. It is used for uniforms, workwear and pocketing, and is often called khaki when it is dyed that colour.

Felt

felt-fabric

Felt is usually a nonwoven: a sheet of wool, hair or fur, sometimes with synthetic fibres, matted together by moisture, heat, pressure and mechanical action. Needle felt, made by entangling synthetic fibres with barbed needles, is a nonwoven too. A woollen cloth woven and then shrunk so heavily that the weave disappears is also called felt. See non-woven fabrics.

Flannel

Flannel Fabric
Flannel Fabric, by Brushy

A medium-weight plain or twill weave, slightly napped on one or both sides, usually wool or cotton. Wool flannel is a suiting cloth; cotton flannel is used for shirts, nightwear and sheets.

Fleece

fleece-knit

A fabric with a thick, soft surface like a sheep’s fleece, made by napping a knitted (or, less often, woven) fabric or by giving it a pile. Sweatshirt fleece is knitted with an extra, thicker yarn on the back that is brushed up. Polar fleece is polyester and is sold in weight classes: Polartec names its own 100 (lightweight), 200 (mid-weight) and 300 (heavyweight).

Foulard

foulard-fabric

A lightweight, lustrous 2/2 twill, usually printed with small figures on a plain ground, in silk, filament polyester or acetate. It is the classic necktie and scarf fabric.

Fustian

fustian-fabric

Originally a cloth with a linen warp and a cotton weft; now a family of heavy cottons with a cut weft pile or a stout weft face, including velveteen, moleskin and corduroy. It was a workwear cloth for centuries.

Gabardine

Gabardine Fabric

A firm, durable, warp-faced twill with a distinct diagonal line at about 45° or 63°, in worsted wool, cotton or polyester. It is used for suits, trousers, uniforms and raincoats. Burberry developed its weatherproof gabardine around 1880.

Gauze

Gauze Fabric

A thin, sheer fabric. In a true gauze weave each weft yarn is gripped by two warp yarns twisted around each other, as in leno, which keeps the open cloth from slipping; cotton surgical gauze is a similar loose cloth. It is used for dressings, curtains and light clothing.

Georgette

Georgette Fabric

A sheer plain-weave crepe with right- and left-twisted crepe yarns in both warp and weft, which gives it a grainy, matt surface and a springy drape. It was first made in silk; most is now polyester. It is a staple sari, blouse and dress fabric.

Gingham

Gingham Fabric

A plain-woven cotton or cotton blend with checks or stripes made by weaving dyed yarns at fixed intervals in both warp and weft, usually one colour and white, so the pattern is the same on both sides. The name came through Dutch from a Malay word usually glossed as striped.

Glass fabric

Fiberglass-Fabric

Fabric woven from yarns of fine glass filaments. Glass does not burn, so it is used for fire blankets and insulation, and as the reinforcement in glass-fibre composites such as boat hulls.

Intarsia

Intarsia-Knit

A weft knit with blocks of colour, each knitted from its own yarn, so there are no floats of unused yarn across the back. Argyle socks and picture sweaters are often intarsia.

Interlock

interlocking-knit

A double weft knit in which long and short needles knit alternately on two beds, giving the effect of two 1×1 ribs crossed into each other. Both faces look like the face of single jersey. It is smooth, stable and does not curl, and is used for T-shirts, polo shirts and babywear.

Jacquard knit

Jacquard-Knit

A weft knit patterned by selecting needles individually, so each yarn colour is knitted only where the design needs it. In a single jersey jacquard the unused yarn floats across the back; in a double jersey jacquard it is knitted into the back as a bird’s eye or striped backing.

Kashmir silk

kashmiri-silk

A regional name for silk fabrics from Kashmir, India, usually plain-woven and embroidered or printed with Kashmiri motifs, used for saris, shirts and stoles.

Khadi

Khadi Fabric

Cloth hand-spun and hand-woven in India, in cotton, silk or wool. Its slightly uneven yarns give it a textured surface. See khadi: hand spinning and weaving.

Khaki

Khaki is a colour, a light yellowish brown, and by extension the cotton or wool cloth dyed that colour for military uniforms and workwear, usually a drill or twill. The word is Urdu for dusty, from a Persian word for dust.

Knitted terry and French terry

knitted-terry

A weft knit with a second yarn that forms loops on one side. Knitted terry is softer and stretchier than woven terry; French terry has small, unbrushed loops on the back and is used for sweatshirts and joggers.

Lamé

A fabric in which flat metallic threads, usually silver or gold, form either the ground or the pattern. It is usually woven, though knitted lamé is also made, and is used for evening wear and stage costumes.

Lawn

A light, thin plain weave of carded or combed cotton, originally linen, with a crisp finish: crisper than voile but not as stiff as organdy. It is used for blouses, handkerchiefs and nightwear. The name probably comes from Laon, in France.

Leno

Leno Fabric

A weave in which the warp yarns work in pairs, one twisted around the other between picks, locking the weft in place. That gives an open fabric firmness and stops the threads sliding. It is used for curtains, mosquito netting and produce sacks, and to bind the edges of cloth on shuttleless looms.

Linsey-woolsey

linsey-woolsey-fabric

A coarse, sturdy cloth woven with a linen warp and a woollen weft, once common in Britain and North America for clothing and bed covers.

Madras

Madras Fabric

A lightweight plain-woven cotton with stripes, checks or plaids in dyed yarns, named after the city of Madras, now Chennai. The Celanese glossary records the trade saying that true madras is guaranteed to bleed: its colours run in the wash and soften with age.

Madras muslin

Madras Muslin Net Fabric

A sheer gauze-woven cotton with figures made by extra weft yarns; after weaving, the floats between the figures are cut away, leaving shorn ends at the edge of each motif. It is a curtain fabric.

Mousseline

Mousseline Fabric

French for muslin: a very fine, light, semi-sheer fabric in silk, wool or cotton. Mousseline de laine is a soft, light, open plain weave of fine worsted, often printed.

Muslin

Muslin Fabric

A broad name for plain-weave cotton or polyester-cotton fabrics, from fine sheers to heavier shirting and sheeting weights. In the United States it is also the plain cotton used to make toiles. The name comes from Mosul, in Iraq, through the Italian mussolina.

Organdy

Organdy Fabric

A very thin, transparent, stiff, wiry cotton muslin. Swiss organdy is chemically treated so that it keeps its crisp, transparent finish through many washes; untreated organdy loses its crispness and has to be starched again. It is used for collars, trims, curtains and bridal wear.

Organza

silk organza
Auckland Museum [ CC BY 4.0 ], via Wikimedia Commons

A stiff, thin, sheer plain weave of silk or of nylon, acrylic or polyester filament, used mainly for evening and bridal wear and for overlays. Silk organza is sold at about 5 to 7.5 momme.

Oxford

Oxford Fabric

A soft but stout shirting in a modified basket weave: a thick, soft weft yarn passes under and over two fine warp yarns together, which gives a slightly textured, two-tone surface. It is usually cotton or polyester-cotton and is the classic button-down shirt fabric.

Percale

percale-fabric

A closely woven plain weave of spun yarns, crisp and matt, used for sheets and dresses. The Celanese glossary gives percale as generally 80 × 80 threads per inch or better, a thread count of 160 or more.

Pointelle

pointelle-knit

A weft knit with a pattern of small holes made by transferring loops to neighbouring needles, which gives a light, lacy effect. It is used for tops, cardigans and babywear. The picture shows embroidered eyelet work, which looks similar; in pointelle the holes are formed by the knitting itself.

Poplin

Poplin Fabric

A plain weave with many more ends than picks, so the fine warp crowds together and the cloth shows a fine rib across its width. Broadcloth is similar, with a finer rib. Cotton and polyester-cotton poplin are standard shirting fabrics, and the ends and picks example above works out the weight of one.

Purl

purl-knit

A weft knit in which alternate courses are drawn through to opposite sides of the fabric, giving horizontal ridges and the same look on both faces. It is thick, stretches lengthwise, and is used for sweaters and children’s wear.

Raschel

raschel-knit

One of the main families of warp knits, with tricot. Raschel machines make lace, nets, power mesh and many other open or textured warp-knitted fabrics.

Rib

rib-knit

A double weft knit in which alternate wales intermesh on the face and the back, so both sides show vertical ribs. It is very elastic across its width and is used for cuffs, collars and waistbands, and for close-fitting tops.

Satin and sateen

Satin Fabric
Satin Fabric, by shaireproductions.com

Both are satin weaves: the face is almost entirely long floats of one set of yarns, with the interlacings spread as far apart as possible, which gives a smooth, lustrous surface. Satin is usually made from filament silk, acetate or polyester; sateen is a satin weave in cotton, common in bed sheets. See also bedsheet fabric types.

Shantung

Shantung Fabric

A plain-woven silk with an unevenly ribbed, slubbed surface and a crisp texture, from irregular yarns such as wild silk or douppioni, which is reeled from double cocoons. It is named after Shandong (Shantung) province in China and is used for bridal and evening wear and furnishings.

Sheeting

Sheeting Fabric

Sheeting is a use: medium-weight, closely woven plain or twill fabrics in cotton, polyester-cotton or linen, made wide enough for bed sheets. Percale and sateen are both sheetings.

Single jersey

flat-jersey-knit

The simplest weft knit, made with a plain stitch on one set of needles, so the loops intermesh in one direction only and the face and back look completely different: V-shaped loops on the face, rows of arcs on the back. It stretches well across its width, curls at cut edges and can ladder. T-shirts, underwear and hosiery are jersey; Two widely sold T-shirts, for example, are knitted from jersey of 145 g/m² and about 180 g/m² (5.3 oz/yd²). The name comes from Jersey, one of the Channel Islands. Its variations are in knitted fabric types.

Sliver knit (high pile)

sliver-knit

A weft knit in which a loose, untwisted rope of fibre (a sliver) is fed to the needles with the ground yarn, so the fibres stand up as a long pile. Imitation fur and many coat linings are made this way, usually from acrylic or modacrylic.

Taffeta

Taffeta fabric
Woven Taffeta Fabric

A crisp, smooth plain weave, usually lustrous, with a fine crosswise rib from a weft slightly heavier than the warp. Silk taffeta is the original; acetate, nylon and polyester are now common. Shot (changeable) and moiré finishes are often applied to it, which is why taffeta is sometimes wrongly described as always having a watered pattern. The name comes from the Persian taftah.

Tartan

Tartan Fabric

A woollen cloth usually woven in a 2/2 twill, with stripes of coloured yarn crossing at right angles. The repeating pattern is called the sett, and the twill is what gives the colours their hatched look where they cross. Tartans are recorded in the Scottish Register of Tartans.

Terry cloth

terry towels
Terry Towels, by Alexas_Fotos

A woven cotton or cotton-blend fabric with uncut loops on one or both sides, made by an extra warp on a dobby or Jacquard loom. The loops give it a large surface for absorbing water. The site’s terry towels article explains how the loops are made.

Ticking

ticking-fabric

A durable, closely woven fabric, usually cotton, for covering mattresses, box springs and pillows. It may be plain, twill or satin woven, usually with strong warp and soft weft yarns, and is often striped.

Tissue

Tissue Fabric

In Indian usage, a light silk or synthetic fabric woven with gold or silver zari in the weft, which gives it a metallic sheen; it is used for saris. Elsewhere, tissue means any very fine, sheer fabric.

Tricot

tricot-knit

The most common type of warp knit, with fine wales on the face and crosswise ribs on the back, usually made from nylon, polyester or acetate filament. It does not ladder, and is used for lingerie, linings and sportswear.

Velour

Knitted-Velour-knit

A fabric with a short, thick pile. Woven velour, in cotton or wool, is used for coats, curtains and upholstery; knitted velour is made like knitted terry with the loops then sheared and brushed, and is used for leisurewear and babywear.

Velvet

velvet fabric
Velvet fabric, by Katelin Elliott

A warp-pile fabric with a short, dense, cut pile. It is woven either as two cloths face to face, with the pile yarns running between them and cut apart by a knife, or over wires that cut the pile loops as they are drawn out. Silk velvet is the original; viscose, cotton and polyester velvets are common. Velveteen, by contrast, has a weft pile. See the complete guide to velvet.

Voile

viole-fabric

A sheer, light, soft plain weave, usually of combed cotton or polyester. It is used for blouses, children’s wear and sheer curtains. Voile is French for veil.

Warp knit

warp-knit

In a warp knit the yarns run along the fabric, fed from beams with one or more yarns for each needle, and each yarn forms loops in neighbouring wales in turn. Warp knits do not ladder and are stable. Tricot and raschel, above, are the main families. See warp knitting and knitted fabric types.

Whipcord

whipcord-fabric

A woven cloth, not a knit: a compact, very steep twill with pronounced round cords running diagonally, in worsted, wool blends or cotton. It is very hard-wearing and is used for uniforms and riding breeches.

Names for a use, a finish or a state, not a type

Some names in fabric lists, including earlier versions of this page, describe what a fabric is for, what has been done to it or how far it has been processed, rather than how it is made. Any of the constructions above can carry them.

Filter fabric

Filter Fabric

A filter fabric is chosen for a job, not made in one way. Filter media are woven, knitted, needle-felted or meltblown, from fibres matched to the temperature and chemicals of the process.

Grey (greige) fabric

cotton-grey-fabric

Grey or greige is a state, not a type: any fabric as it comes off the loom or knitting machine, before scouring, bleaching, dyeing or finishing. The word has nothing to do with colour. Mills sell and price much of their cloth in the greige state.

Industrial fabric

Industrial Fabric

An older term for fabrics made for performance rather than appearance, often from glass, carbon, aramid or high-tenacity polyester and nylon. They are now called technical textiles; see types of technical textiles.

Laminated fabric

Laminated Fabric

A laminated fabric is a fabric bonded to a film, a foam or a second fabric, or a reinforcing scrim sealed between two layers of plastic film. A waterproof breathable membrane laminated to a shell fabric is a common example. See coated and laminated textile fabrics.

Narrow fabric

Narrow Fabric

Narrow fabrics are woven, knitted or braided fabrics made in narrow widths: tapes, ribbons, labels, webbing, elastic and zip tapes. See narrow fabrics.

Plain weave

Plain Weave Fabrics
Plain weave fabric, by Abby Lanes

Plain describes a weave, not a fabric: each weft passes over one warp and under the next, and the next weft does the reverse. Poplin, voile, chiffon, taffeta and canvas are all plain weaves. See plain weaves.

Quilted fabric

Quilted Fabric
Quilted Fabric, by PublicDomainPictures

Quilting is a construction of layers: a padding such as down or fibrefill between two fabrics, held in place by stitching or by sealing in a regular pattern. It is used for quilts, jackets, mattress tops and bags.

Reflective fabric

Reflective Fabric

A fabric coated or laminated with retroreflective glass beads or microprisms, which send light back towards its source. It is used on high-visibility workwear and safety clothing.

Stretch fabric

Stretch Fabric

A stretch fabric is any woven or knitted fabric made with elastane (spandex) or textured yarns so that it stretches and recovers in one direction or both. See spandex fabric.

Download the list as a PDF

The printable version, 87 types of fabric and their patterns (PDF, 1 MB), has a picture and a description of each fabric, one or two to a page, for classrooms and offline reading. It was first published in 2010. Where it and this page differ, this page is the corrected version.

Sources

Every source below was read on 5 October 2026. Standards are cited to their catalogue entries and to the records on this site, which give scope and context but never reproduce a standard’s text. Definitions are this site’s own wording, checked against the glossaries and dictionaries listed.

Change log. 5 October 2026: rewritten in full, with the fibre classification that was on a separate page added. Corrected from the previous version: whipcord is a woven twill, not a knit; tartan is usually a 2/2 twill, not a plain weave; damask is a flat, reversible Jacquard, not a heavy, rough fabric; in denim the dyed warp shows on the face; cambric is named after Cambrai, not Cambria; the Aertex company dates from 1888, and no 1886 patent could be found; baize is a napped woollen, later also cotton, cloth rather than a wool-cotton blend; satin is woven, not knitted; the watered (moiré) look is a finish sometimes given to taffeta, not a feature of all taffeta; the claim that red reflects light best was removed; and nine names that describe a use, a finish or a state (filter, greige, industrial, laminated, narrow, plain, quilted, reflective and stretch) are now listed separately from the fabric types. The worked examples use this site’s calculators as they stood on this date.

Found an error? Please tell us through the contact page, naming the fabric and the source that disagrees.

72 comments

  1. Viviana Hicks

    Hi there! Just wanted to let you know how much I enjoyed reading this post. Your approach to the subject was unique and informative. It’s clear that you put a lot of effort into your writing. Keep up the great work, and I can’t wait to see what else you have in store.

  2. Guanghong Nonwoven

    I thoroughly enjoyed reading this article. It describes this subject very effectively. I am really enjoying the blog and will bookmark it! Keep writing interesting articles! Thank you for sharing this informative blog.

  3. Nayan Prime

    Textile

    These all are trusted and leading companies in surat which can be helpful to guide reports of Top Fabrics and Textile products companies from Surat City. The silk manufacturing companies in Surat are at all-time high levels.

  4. nayan parmar

    Double Bed Blanket
    Quilts can be used for Often antique quilts are used to make doll clothing or reupholster furniture. something from mattress protecting to wall decorations. The versatility of quilts additionally lends itself. made from down feathers because of its usefulness as a thermal insulator.

  5. This is a very powerful article. Almost all different types of fabric are described here. It will be very helpful for those who are learning or working in the textile sector. Thanks a lot for this wonderful article.

  6. Another type of fiberglass fabrics are broadly used for thermal insulation, for smoke and fire protective clothing and equipment, for acoustic solutions and reinforcement in building and construction sector. Find out more about them here: https://www.valmiera-glass .com/en/product-world/products/technical-fabrics/

  7. It will be very helpful for those who are learning or working in textile sector. Thank a lot for this wonderful article. I think visitors will get some significant information visiting through the link given below.

  8. Shakil Ahmed

    Very helpful for knowing some kind of fabric. It is very helpful for who wants to be a merchandiser.
    Thanks for sharing.

  9. Rudolph Roof

    It is so interesting i was searching for this topic from a long time. I read this article very carefully and now I got all my best information for writing blog on acrylic tissue box suppliers . I am so glad that i finally find blog resemblance to my topic. Thanks for this.

  10. Textile School Editor

    Thank you for your kind words.
    RSS link: https://textileschool.com/feed/
    Subscribing to our newsletters will help you receiving the newsletters in your mailbox. We won’t spam.

  11. I’m currently engaged in the fabrics trade sector. So this website is quite useful for the knowledge foundation of fabrics. Higly appreciative

  12. Textile Trick

    Nice post sir thanks for sharing

    //www.textiletrick.com” title=”Textile Trick ” rel=”nofollow ugc”>Textile Trick

  13. Would you mind explainING the difference between fabric that cost 15.00 a yard and 250.00 a yard. I’ve been sewing for over fifty years and have been discouraged by the prices for curtain fabrics and so on . Even 25.00 and yard kills me because I like to do 3 widths and have huge windows. I get “name has something to do with it, but for heavens sakes , how much. They sure took the fun out sewing. I like buying the good stuff but who could rationalize 250.000 a yard for curtain fabric.

  14. Rebecca Kramer

    Hi, Thanks for sharing very essential stuff. I am new in the textile and fabrics industry. I have learned a lot of things from this article. Recently I have started an online store for selling different types of fabrics. I think this post will be very useful for the newbie in the industry of textile and fabrics.

    1. Am interested in fabric as a business, though I do a little of it now but I really want to do different types of fabric as business. need help pls

  15. I am starting out my own T-Shirt brand and would like to know what is best fabric one can use for T-Shirts as quality is a priority?

  16. Choosing the right fabrics is an important thing, and at the same time quite difficult when we choose the fabric for the first time. A very nice guide. Certainly many people will benefit from your advice.

  17. Can you please list the fabrics denim, chiffon, organza, velvet, and taffeta from most flexible to least flexible.

  18. Textile Teacher

    For a ‘School of Textiles’, some of the information outlined in this article is inaccurate & would be very confusing for students. Here are just a few of the questionable items. * Students need to know that there is a difference between FIBRES (Australian spelling) and FABRICS. These two terms are not synonymous. Fibres are the building blocks of all fabrics & classified into 3 groups (natural – eg: cotton, wool, silk, linen, jute, hemp etc) man-made or synthetic (eg:nylon, polyester, acrylic, rayon, acetate etc) and mineral (eg asbestos & fibreglass). Fibres most often have to be SPUN together in yarns before they can be made into fabrics. Woollen fibres are an exception. Wool fibres can be matted or felted together to form fabrics (eg: like felts used for the walls of yurts). Fabrics result from the combining of the fibres. Fabrics are made through either weaving, knitting, matting fibres together. There are many other construction methods used for making industrial use fabrics. Nowhere is this clarification between fibres & fabrics made. ** No disadvantages are given of the fabrics mentioned. For example, fabrics made of cotton are very flammable, even more so when woven fabrics made of cotton are brushed (eg: flannelette) of are flowing in design. That is why in Australia there is very strict labelling of childrens’ nightwear so people are aware of the dangers of this type of fibre/fabric combination. Linen is expensive & wrinkles badly (needs ironing). Wool is not really very strong as this article states – in fact it is the weakest of the natural fibres. You would never find mens suits made out of 100% wool as the woollen fibre is not strong enough. There would be bagging and sagging at the seat, knees & elbows of the garment. *** The bit about ‘grey fabric’… wow in all of my years as a textile teacher, I’ve never heard of it, seen it or seen any reference to it. I think this bit on ‘grey fabric’ is a furphy! Sounds like a student trying to fluff their way through an exam question… lots of words but no substance! **** Satin is a type of woven fabric that has ‘floating’ warp yarns. It is this type of woven construction that gives satin fabric lustre & not just the type of fibre used.***** Stretch fabrics can result from a) using a knitted fabric construction eg socks b) using fabric draped on the bias (using the 45 degree angle of the warp & weft yarns c) introducing an elastomeric yarn into the fabric construction eg 5% elastomeric yarns to denim weave for stretch jeans. ***** calling polyester a fabric is confusing for your students. Polyester is a fibre. It can then be woven or knitted to make a polyester fabric.**** I agree with the John, the term nylon did not come about as stated in this article. As this written piece is on your site titled “Textile School” it needs to be more accurate & less confusing to your students. This article needs to be proof-read by a teacher of textiles & corrected. References would also give it more credibility.

  19. anybody ever gave tide pods a try give me a rate 1-10 i am thinking about giving them a go they just look so good:)

  20. This helped me a lot at my school project. Thank you who ever posted this i love textile . Thank you so much for helping me out

  21. Ishita Yadav

    This was very useful. Thankyou.
    Also, I needed a brief on PST fabric, which I have commonly heard of being used as a substitute of Chanderi by Indian retailers. Would be very helpful. 🙂

  22. OK…BUT As I mentioned to the webmaster, the name Nylon most certainly does not come from a combining of the the New York/London (NY-LON) names. Dupont, the inventors and patent holders for Nylon state that the name is as synthetic as the fiber. They took the random syllable Nyl and combined it with the “on” (as in Ray”on” or Cott”on”) to make it sound fabric-like. Although the idea that it is New York and London combined is interesting, it makes no sense since Dupont is based in Delaware and really has no major ties to either of those cities…so why randomly name it after both? Why not Bogata and Tokyo for that matter? (Botok?) Another case of “saw it on the web so it must be true” uncovered as false.

  23. This list is super!!! Thank you. I have a question. I am making a pincushion specifically for the regular session to session sharpening of needle nose tweezers while I work applying eyelash extensions. The pincushion will be filled with emery, a finely ground metal used for sharpening needles, pins and tools. As for the fabric cover, I need it to be durable and mainly lint free. But have enough texture and body to it, a little grit to it even, so that when I pass my tweezers through it into the emery, the small bits of eyelash glue (similar to superglue in strength but flakier in texture and strength), can slough off onto fabric and off of my tweezers. Please any help with this question would be greatly appreciated!

    ….thinking heavy cotton canvas, wool, a jute weave, or a poly/wool blend…

  24. CA Pawan Kr Agrawal, Kolkata.

    Interlining is a very important in apparel manufacturing. Interlining is one kind of accessories that is used
    between the two layers of fabric in a garment. To keep the different component or part of apparel in a desired shape, a kind of fabric is used between the two ply of fabric by sewing or fusing is called interlining. Generally, interlinings are soft, thick, and flexible. Interlining is generally used in collar, cuffs, waist band, front facing of coat, outerwear plackets, jackets, blazers etc.
    Fusible Interlining:
    It is most used interlining. The interlining which is used between two layers of fabrics by applying heat and
    pressure for a certain time is called Fusible Interlining. Fusible interlining is used for all kinds of apparel. Also it is used in “Ready to wear” and “Bespoke garment”. It is very popular.

    My question is whether character of textile fabrics is retained or lost after applying HDPE or LDPE by heat process on one side of cotton fabrics?

  25. Isabeaumonde

    I’m sad to see some serious inaccuracies here. The biggest is the listing of Rayon as a synthetic. It is an organic material processed as a synthetic, which does not change it’s organic properties. Chiffon, organza….both historically silk.

    1. Paper is a man made cellulose material similar to Rayon fabric. Methods of manufacturing and applications are different and can not replace each other though both are made from same source of raw material i.e. wood pulp. Fabric needs air permeability, flexibility and durability that can not be achieved in paper form. However non-woven Rayon fabric is similar to paper.

      Fabric can also make like paper by applying paper finish on it where both objectives can be met if required.

  26. Dagmar Kugler

    Can you tell me if Ramie is washable? I have a hand me down Spring Jacket made of Polyester and Rani (misspelled on item?, unless this is a mystery fabric). It smells old and stored, but looks brand new. Love the site btw., very informative.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device

The Selvedge · free · one email a week

Know what changed in textiles this week.

Our register tracks 3,130 textile standards. Nobody reads them all, so once a week we tell you which ones moved, and what else is new.

  • Standards added, revised or withdrawn that week
  • One textile calculation, worked through to its answer
  • New and revised guides on the site
  • Textile fairs coming up, with their dates

Free when you confirm: Spinning and Weaving Calculations (PDF). 49 calculations, from the blowroom to the loom, each with its formulas and a worked example.

We send a confirmation link first. Unsubscribe in one click, any time.

  • No spam
  • Your address is not shared
  • Unsubscribe in one click